General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.66 g/cm³ Show Supplier Material materials with Densidad of 2.66 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 75 - 80 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 75 - 80 [-] | Test method: 2.5/62.5 |
Elongación | 23.0 °C | 18 - 25 % Show Supplier Material materials with Elongación of 18 - 25 % | |
Límite elástico Rp 0,2 | 23.0 °C | 115 - 130 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 115 - 130 MPa | |
Módulo elástico | 23.0 °C | 70 GPa Show Supplier Material materials with Módulo elástico of 70 GPa | |
Resistencia a la tracción | 23.0 °C | 250 - 280 MPa Show Supplier Material materials with Resistencia a la tracción of 250 - 280 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 900 J/(kg·K) Show Supplier Material materials with Calor específico of 900 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 2.33E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.33E-5 1/K |
Conductividad térmica | 23.0 °C | 110 - 130 W/(m·K) Show Supplier Material materials with Conductividad térmica of 110 - 130 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.60E+7 - 1.80E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.60E+7 - 1.80E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Non heat treatable | |
Processing history | Temper: O3 |