General
Medidas
Property | Value |
---|---|
Ancho | 1540 mm Show Supplier Material materials with Ancho of 1540 mm |
Dimensions | Standard stock sizes: 1540mm x 3048mm and 20-570mm in thickness |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 110 - 120 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 110 - 120 [-] | Test method: 2.5/62.5 |
Elongación A5 | 23.0 °C | 2.5 - 4.5 % Show Supplier Material materials with Elongación A5 of 2.5 - 4.5 % | |
Límite elástico Rp 0,2 | 23.0 °C | 290 - 340 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 290 - 340 MPa | |
Módulo elástico | 23.0 °C | 70 GPa Show Supplier Material materials with Módulo elástico of 70 GPa | |
Resistencia a la tracción | 23.0 °C | 320 - 380 MPa Show Supplier Material materials with Resistencia a la tracción of 320 - 380 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 875 J/(kg·K) Show Supplier Material materials with Calor específico of 875 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 2.3E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.3E-5 1/K |
Conductividad térmica | 23.0 °C | 125 - 155 W/(m·K) Show Supplier Material materials with Conductividad térmica of 125 - 155 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.10E+7 - 2.40E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 2.10E+7 - 2.40E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Heat treatable alloy | |
Processing history | Temper: T79, solution heat treated and artificially aged |