General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.8 g/cm³ Show Supplier Material materials with Densidad of 2.8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 110 - 115 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 110 - 115 [-] | Test method: 2.5/62.5 |
Elongación | 23.0 °C | 5 - 8 % Show Supplier Material materials with Elongación of 5 - 8 % | |
Límite elástico Rp 0,2 | 23.0 °C | 290 - 330 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 290 - 330 MPa | |
Módulo elástico | 23.0 °C | 70 GPa Show Supplier Material materials with Módulo elástico of 70 GPa | |
Resistencia a la tracción | 23.0 °C | 350 - 370 MPa Show Supplier Material materials with Resistencia a la tracción of 350 - 370 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 875 J/(kg·K) Show Supplier Material materials with Calor específico of 875 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 2.33E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.33E-5 1/K |
Conductividad térmica | 23.0 °C | 125 - 155 W/(m·K) Show Supplier Material materials with Conductividad térmica of 125 - 155 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.10E+7 - 2.40E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 2.10E+7 - 2.40E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Non heat treatable | |
Processing history | Temper: T79 |