General
Property | Value | Comment |
---|---|---|
Densidad | 1.98 - 2.38 g/cm³ Show Supplier Material materials with Densidad of 1.98 - 2.38 g/cm³ | loose pack density |
Densidad aparente | 2.11 - 2.54 g/cm³ Show Supplier Material materials with Densidad aparente of 2.11 - 2.54 g/cm³ | ANSI B74.4 |
Tamaño de los cristales | 17.0 μm Show Supplier Material materials with Tamaño de los cristales of 17.0 μm | |
True particle density | 4.6 g/cm³ Show Supplier Material materials with True particle density of 4.6 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 1900.0 °C Show Supplier Material materials with Temperatura de fusión of 1900.0 °C |
Chemical properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Aluminio | 75 % Show Supplier Material materials with Aluminio of 75 % | ANSI B74.14 | max. Al₂O₃ |
Azufre | 0.06 % Show Supplier Material materials with Azufre of 0.06 % | ANSI B74.14 | |
Calcio | 0.1 % Show Supplier Material materials with Calcio of 0.1 % | ANSI B74.14 | CaO |
Circonio | 23 % Show Supplier Material materials with Circonio of 23 % | ANSI B74.14 | ZrO₂ |
Hierro | 0.3 % Show Supplier Material materials with Hierro of 0.3 % | ANSI B74.14 | Fe₂O₃ |
Magnesio | 0.03 % Show Supplier Material materials with Magnesio of 0.03 % | ANSI B74.14 | MgO |
Silicona | 0.3 % Show Supplier Material materials with Silicona of 0.3 % | ANSI B74.14 | SiO₂ |
Sodio | 0.08 % Show Supplier Material materials with Sodio of 0.08 % | ANSI B74.14 | Na₂O |
Titanio | 0.4 % Show Supplier Material materials with Titanio of 0.4 % | ANSI B74.14 | TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Alumina Zirconia 25% is used primarily for producing large grinding wheels for foundry snagging and track grinding. It is also an excellent blasting material for granite and other materials where long life is required, as well as in some refractory applications. |