Material: el 'APTIV® 1000 Series Film 125µm' que buscabas ha sido remplazado por el material siguiente.

APTIV® 1000 Series Film 125µm

Nombres alternativos y comerciales
APTIV® 1000 Series Film 125µm
Want to keep this datasheet? Save it now in your required format

Description

APTIV® 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.


APTIV films are a comprehensive range of versatile, high-performance films, the use of which can facilitate reduced systems costs, improved performance and enhanced design freedom.


APTIV 1000 has a unique combination of properties providing high temperature performance, lightweight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, wear and abrasion resistance, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen-free and ease of processing makes APTIV films a technology enabler for our customers and end users.

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

Medidas

PropertyValue

Espesor

0.13 mm

Show Material materials with Espesor of 0.13 mm

Mecánica

PropertyTemperatureValueComment

Elongación

23.0 °C

150 %

Show Material materials with Elongación of 150 %

ISO 527

Elongación transversal

23.0 °C

150 %

Show Material materials with Elongación transversal of 150 %

ISO 527

Módulo elástico

23.0 °C

2.3 GPa

Show Material materials with Módulo elástico of 2.3 GPa

ISO 527

Módulo elástico transversal

23.0 °C

2.3 GPa

Show Material materials with Módulo elástico transversal of 2.3 GPa

ISO 527

Resistencia a la tracción

23.0 °C

120 MPa

Show Material materials with Resistencia a la tracción of 120 MPa

ISO 527

Resistencia a la tracción transversal

23.0 °C

120 MPa

Show Material materials with Resistencia a la tracción transversal of 120 MPa

ISO 527

Eléctrico

PropertyTemperatureValueComment

Rigidez dieléctrica

23.0 °C

120 kV/mm

Show Material materials with Rigidez dieléctrica of 120 kV/mm

ASTM D149 (6.25mm electrode)

Tensión de ruptura

23.0 °C

15 kV

Show Material materials with Tensión de ruptura of 15 kV

ASTM D149 (6.25mm electrode)

Technological properties

Property
Application areas

Electrical insulation, pressure sensitive tapes, printed circuit substrates, high temperature labels, washers in high speed motors, washers in mobile phone hinges, flexible surface heaters, aerospace insulation, pressure sensor membranes, acoustic speaker diaphragms, capacitors, composites, proven temperature resistance to use of lead free solders

Certifications

APTIV® film is FDA and EU approved for food contact and is RoHS and 3A Sanitary Standards compliant.

Other

The key features are: High heat resistance, excellent tribological properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent barrier properties, excellent acoustic properties, high purity, lightweight, recyclable, easy to process

Processing methods

Can be laminated to other materials thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated.