APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.


APTIV films are a comprehensive range of versatile, high-performance films, the use of which can facilitate reduced systems costs, improved performance and enhanced design freedom.


APTIV 1100 has a unique combination of properties providing high temperature performance, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen-free and ease of processing makes APTIV films a technology enabler for our customers and end users.


APTIV 1100 series provides a higher modulus and lower coefficient of linear thermal expansion over the APTIV 1000 series.

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

Medidas

PropertyValue

Espesor

0.05 mm

Show Material materials with Espesor of 0.05 mm

Mecánica

PropertyTemperatureValueComment

Elongación

23.0 °C

10 %

Show Material materials with Elongación of 10 %

ISO 527

Elongación transversal

23.0 °C

10 %

Show Material materials with Elongación transversal of 10 %

ISO 527

Módulo elástico

23.0 °C

5.5 GPa

Show Material materials with Módulo elástico of 5.5 GPa

ISO 527

Módulo elástico transversal

23.0 °C

4.5 GPa

Show Material materials with Módulo elástico transversal of 4.5 GPa

ISO 527

Resistencia a la tracción

23.0 °C

90 MPa

Show Material materials with Resistencia a la tracción of 90 MPa

ISO 527

Resistencia a la tracción transversal

23.0 °C

90 MPa

Show Material materials with Resistencia a la tracción transversal of 90 MPa

ISO 527

Technological properties

Property
Application areas

Electrical insulation, printed circuit substrates, high temperature labels, flexible surface heaters, proven temperature resistance to use of lead free solders, acoustic speaker diaphragms, pressure sensor membranes

Certifications

APTIV® film is FDA and EU approved for food contact and is RoHS compliant.

Other

The key features are: High heat resistance, broad chemical resistance, excellent barrier properties, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent acoustic properties, high purity, lightweight, recyclable, easy to process. The APTIV 1100 series offers an improved thermal conductivity over APTIV 1000 films.

Processing methods

Can be laminated to other materials, thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated.