Material: el 'APTIV® 2000 Series Film 50µm' que buscabas ha sido remplazado por el material siguiente.

APTIV® 2000 Series Film 50µm

Nombres alternativos y comerciales
APTIV® 2000 Series Film 50µm
Want to keep this datasheet? Save it now in your required format

Description

APTIV® 2000 series films are the unfilled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.


APTIV films are a comprehensive range of versatile, high-performance films, the use of which can facilitate reduced systems costs, improved performance and enhanced design freedom.


APTIV 2000 has a unique combination of properties providing high temperature performance, lightweight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, wear and abrasion resistance, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen-free and ease of processing makes APTIV films a technology enabler for our customers and end users.


Please note - APTIV 2000 will crystallise if taken above the Tg [143°C (289°F)] in either secondary processes or end use application. The crystallisation is not reversible back to the amorphous phase without re-melting the material. Consideration of the temperature range during processing and end use application needs to be included if selecting APTIV 2000.

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValueComment

Absorción de agua

23.0 °C

0.21 %

Show Material materials with Absorción de agua of 0.21 %

ISO 62 (50% RH, 24h)

Densidad

23.0 °C

1.26 g/cm³

Show Material materials with Densidad of 1.26 g/cm³

ISO 1183

Medidas

PropertyValue

Espesor

0.05 mm

Show Material materials with Espesor of 0.05 mm

Mecánica

PropertyTemperatureValueComment

Elongación

23.0 °C

200 %

Show Material materials with Elongación of 200 %

ISO 527

Elongación transversal

23.0 °C

200 %

Show Material materials with Elongación transversal of 200 %

ISO 527

Módulo elástico

23.0 °C

1.8 GPa

Show Material materials with Módulo elástico of 1.8 GPa

ISO 527

Módulo elástico transversal

23.0 °C

1.8 GPa

Show Material materials with Módulo elástico transversal of 1.8 GPa

ISO 527

Resistencia a desgarros

23.0 °C

6 kN/m

Show Material materials with Resistencia a desgarros of 6 kN/m

ISO 6383-1

Resistencia a desgarros transversal

23.0 °C

6 kN/m

Show Material materials with Resistencia a desgarros transversal of 6 kN/m

ISO 6383-1

Resistencia a la perforación

23.0 °C

470 kJ/m²

Show Material materials with Resistencia a la perforación of 470 kJ/m²

Def Stan 81-75

Resistencia a la tracción

23.0 °C

120 MPa

Show Material materials with Resistencia a la tracción of 120 MPa

ISO 527

Resistencia a la tracción transversal

23.0 °C

120 MPa

Show Material materials with Resistencia a la tracción transversal of 120 MPa

ISO 527

Aplicaciones térmicas

PropertyTemperatureValueComment

Coeficiente de dilatación térmica

23.0 °C

6E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 6E-5 1/K

ASTM D696 (below Tg)

Temperatura de transición del vidrio

143 °C

Show Material materials with Temperatura de transición del vidrio of 143 °C

Eléctrico

PropertyTemperatureValueComment

Constante dieléctrica

23.0 °C

3 [-]

Show Material materials with Constante dieléctrica of 3 [-]

ASTM D150 (10MHz)

Resistividad eléctrica

23.0 °C

2.00E+14 Ω·m

Show Material materials with Resistividad eléctrica of 2.00E+14 Ω·m

ASTM D257 (100V)

Rigidez dieléctrica

23.0 °C

190 kV/mm

Show Material materials with Rigidez dieléctrica of 190 kV/mm

ASTM D149 (6.25mm electrode)

Tangente de pérdidas

23.0 °C

3E-3 [-]

Show Material materials with Tangente de pérdidas of 3E-3 [-]

ASTM D150 (10Mhz)

Tensión de ruptura

23.0 °C

9.5 kV

Show Material materials with Tensión de ruptura of 9.5 kV

ASTM D149 (6.25mm electrode)

Rheological Properties

PropertyTemperatureValueComment

Contracción

200.0 °C

10 %

Show Material materials with Contracción of 10 %

TM-VX-84

Contracción transversal

200.0 °C

5 %

Show Material materials with Contracción transversal of 5 %

TM-VX-84

Technological properties

Property
Application areas

Aerospace insulation, electrical insulation, acoustic speaker diaphragms, thermoforming of thin wall parts, composites

Certifications

APTIV 2000 film is approved for Food Contact Use: APTIV 2000 film is compliant with the compositional requirements of FDA 21 CFR 177.2415. APTIV 2000 film is compliant with the framework regulation (EC) No. 1935/2004/EC and commission directive 2002/72/EC and the amendments up to 2005/79/EC. APTIV 2000 film is fully compliant with the 3-A Sanitary Standards. APTIV film 2000 complies with the requirements of RoHS European Directive 2002/95/EC and can be used to manufacture products compliant with the same directive. APTIV 2000 film is inherently halogen-free in accordance with IEC61249-2-21.

Other

The key features are: High heat resistance, excellent Flexural fatigue properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent acoustic properties, high purity, lightweight, recyclable, easy to process.

Processing methods

Can be laminated to other materials thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated. APTIV 2000 film can easily be subjected to a range of secondary process operations, which allow designers and engineers to obtain the benefits of APTIV film properties in a variety of forms: Surface treatment, adhesion, coatings, slitting, die cutting and stamping, thermal lamination, heat welding and heat sealing, metallisation, laser marking and machining, thermoforming, printing