Material: el 'Polyvinylidenefluoride (PVDF) Granules (FV306300)' que buscabas ha sido remplazado por el material siguiente.

Kynar Flex® 2800-00

Nombres alternativos y comerciales
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® resins are fluorinated thermoplastic copolymers.

Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo-mechanical properties.

Kynar Flex® 2800-00 resin is a standard grade of granules, compared to the homopolymer grades, which exhibits a lower modulus, a better resistance to stress cracking in alkaline and oxidizing media, and a lower melting point. For cable coating, extrusion of tube and plaque, compression molding of bulky parts.

Additional characteristics:

  • Easily processed using conventional equipment
  • Excellent thermal stability
  • Retains properties after aging
  • Pigmentable
  • UL RTI temperature rating 125ºC
  • Radiation crosslinking

  • Los datos sobre este material han sido proporcionados por Arkema Technical Polymers.

    A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
    Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Propiedades

    General

    PropertyValueTesting StandardConditionComment

    Absorción de agua

    0.03 %

    Show Supplier Material materials with Absorción de agua of 0.03 %

    Sim. to ISO 62

    0.03 - 0.05 %

    Show Supplier Material materials with Absorción de agua of 0.03 - 0.05 %

    ASTM D570

    Coefficient of friction

    0.33 [-]

    Show Supplier Material materials with Coefficient of friction of 0.33 [-]

    ASTM D1894

    vs Steel, Static

    0.33 [-]

    Show Supplier Material materials with Coefficient of friction of 0.33 [-]

    ASTM D1894

    vs Steel, Kinetic

    Densidad

    1.77 - 1.8 g/cm³

    Show Supplier Material materials with Densidad of 1.77 - 1.8 g/cm³

    ASTM D792

    1.78 g/cm³

    Show Supplier Material materials with Densidad of 1.78 g/cm³

    ISO 1183

    dry

    Moisture absorption

    0.015 %

    Show Supplier Material materials with Moisture absorption of 0.015 %

    Sim. to ISO 62

    Índice límite de óxigeno

    42 %

    Show Supplier Material materials with Índice límite de óxigeno of 42 %

    ASTM D2863

    43 %

    Show Supplier Material materials with Índice límite de óxigeno of 43 %

    ISO 4589-1/-2

    dry

    Mecánica

    PropertyTemperatureValueTesting StandardConditionComment

    Dureza Shore D

    60 - 70 [-]

    Show Supplier Material materials with Dureza Shore D of 60 - 70 [-]

    ASTM D2240

    Elongación

    50 %

    Show Supplier Material materials with Elongación of 50 %

    ISO 527-1/-2

    dry

    min. | nominal

    100 - 300 %

    Show Supplier Material materials with Elongación of 100 - 300 %

    ASTM D638

    Elongation at yield

    10 - 20 %

    Show Supplier Material materials with Elongation at yield of 10 - 20 %

    ASTM D638

    15 %

    Show Supplier Material materials with Elongation at yield of 15 %

    ISO 527-1/-2

    dry

    Impact strength, Charpy notched, ASTM

    23 °C

    534 - 1070 J/m

    Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 534 - 1070 J/m

    ASTM D256

    Impact strength, Charpy unnotched, ASTM

    No Break at 23°C

    ASTM D256

    Límite elástico

    20 - 34.5 MPa

    Show Supplier Material materials with Límite elástico of 20 - 34.5 MPa

    ASTM D638

    27 MPa

    Show Supplier Material materials with Límite elástico of 27 MPa

    ISO 527-1/-2

    dry

    Módulo de flexión

    0.483 - 0.758 GPa

    Show Supplier Material materials with Módulo de flexión of 0.483 - 0.758 GPa

    ASTM D790

    Módulo elástico

    0.552 - 0.896 GPa

    Show Supplier Material materials with Módulo elástico of 0.552 - 0.896 GPa

    ASTM D638

    0.7 GPa

    Show Supplier Material materials with Módulo elástico of 0.7 GPa

    ISO 527-1/-2

    dry

    Resistencia a la compresión

    31 - 41.4 MPa

    Show Supplier Material materials with Resistencia a la compresión of 31 - 41.4 MPa

    ASTM D695

    Resistencia a la flexión

    20.7 - 34.5 MPa

    Show Supplier Material materials with Resistencia a la flexión of 20.7 - 34.5 MPa

    ASTM D790

    at 5% strain

    Resistencia a la tracción

    17.2 - 34.5 MPa

    Show Supplier Material materials with Resistencia a la tracción of 17.2 - 34.5 MPa

    ASTM D638

    Resistencia al choque, ensayo Charpy entallado

    -30 °C

    5 kJ/m²

    Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m²

    ISO 179/1eA

    dry

    No Break at 23°C

    Aplicaciones térmicas

    PropertyValueTesting StandardConditionPressureComment

    Calor específico

    745 - 958 J/(kg·K)

    Show Supplier Material materials with Calor específico of 745 - 958 J/(kg·K)

    DSC

    Coeficiente de dilatación térmica

    0.000126 - 0.000185 1/K

    Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000126 - 0.000185 1/K

    ASTM D696

    0.00016 1/K

    Show Supplier Material materials with Coeficiente de dilatación térmica of 0.00016 1/K

    ISO 11359-1/-2

    dry

    Conductividad térmica

    0.144 - 0.18 W/(m·K)

    Show Supplier Material materials with Conductividad térmica of 0.144 - 0.18 W/(m·K)

    ASTM D433

    Relative temperature index, electrical

    130 °C

    Show Supplier Material materials with Relative temperature index, electrical of 130 °C

    UL 746B

    Relative temperature index, mechanical strength

    130 °C

    Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C

    UL 746B

    Temperatura de flexión bajo carga

    40 - 55 °C

    Show Supplier Material materials with Temperatura de flexión bajo carga of 40 - 55 °C

    ASTM D648

    2 MPa

    248 °F/hr

    48 °C

    Show Supplier Material materials with Temperatura de flexión bajo carga of 48 °C

    ISO 75-1/-2

    dry

    2 MPa

    60 - 75 °C

    Show Supplier Material materials with Temperatura de flexión bajo carga of 60 - 75 °C

    ASTM D648

    0.45 MPa

    248 °F/hr

    68 °C

    Show Supplier Material materials with Temperatura de flexión bajo carga of 68 °C

    ISO 75-1/-2

    dry

    0.45 MPa

    Temperatura de fusión

    140 - 145 °C

    Show Supplier Material materials with Temperatura de fusión of 140 - 145 °C

    ASTM D3418

    143 °C

    Show Supplier Material materials with Temperatura de fusión of 143 °C

    ISO 11357-1/-3

    dry

    10°C/min

    Temperatura de reblandecimiento Vicat

    79 °C

    Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 79 °C

    ISO 306

    50°C/h 50N

    Temperatura de transición del vidrio

    -41.1 - -39.4 °C

    Show Supplier Material materials with Temperatura de transición del vidrio of -41.1 - -39.4 °C

    ASTM D7028

    -40 °C

    Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C

    ISO 11357-1/-2

    dry

    10°C/min

    Thermal decomposition in air

    375 °C

    Show Supplier Material materials with Thermal decomposition in air of 375 °C

    TGA

    1% wt. loss

    Thermal decomposition in nitrogen

    410 °C

    Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C

    TGA

    1% wt. loss

    Inflamabilidad

    At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 and yellow card available

    Eléctrico

    PropertyValueFrequencyTesting StandardCondition

    Constante dieléctrica

    3.5 - 10.6 [-]

    Show Supplier Material materials with Constante dieléctrica of 3.5 - 10.6 [-]

    1KHz

    ASTM D150

    7 [-]

    Show Supplier Material materials with Constante dieléctrica of 7 [-]

    1MHz

    IEC 60250

    dry

    11 [-]

    Show Supplier Material materials with Constante dieléctrica of 11 [-]

    100Hz

    IEC 60250

    dry

    Factor de disipación

    0.02 - 0.21 [-]

    Show Supplier Material materials with Factor de disipación of 0.02 - 0.21 [-]

    100KHz

    ASTM D150

    0.052 [-]

    Show Supplier Material materials with Factor de disipación of 0.052 [-]

    100Hz

    IEC 60250

    dry

    0.233 [-]

    Show Supplier Material materials with Factor de disipación of 0.233 [-]

    1MHz

    IEC 60250

    dry

    Rigidez dieléctrica

    51.2 - 59.1 kV/mm

    Show Supplier Material materials with Rigidez dieléctrica of 51.2 - 59.1 kV/mm

    ASTM D149

    Surface resistivity

    5.1e+11 - 5.3e+11 Ω/sq

    Show Supplier Material materials with Surface resistivity of 5.1e+11 - 5.3e+11 Ω/sq

    ASTM D257

    Volume resistivity

    2e+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm

    ASTM D257

    65% RH

    2e+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm

    IEC 60093

    dry

    Óptico

    PropertyValueTesting StandardComment

    Índice de refracción

    1 [-]

    Show Supplier Material materials with Índice de refracción of 1 [-]

    ASTM D542

    sodium D line

    Rheological Properties

    PropertyValueTesting StandardConditionComment

    Melt viscosity

    2700 - 220000 Pa·s

    Show Supplier Material materials with Melt viscosity of 2700 - 220000 Pa·s

    ASTM D3835

    Velocidad de flujo de la masa derretida

    3 - 8 g/10min

    Show Supplier Material materials with Velocidad de flujo de la masa derretida of 3 - 8 g/10min

    ASTM D1238

    230°C/12.5kg

    Velocidad de flujo del volumen derretido

    0.5 cm³/10min

    Show Supplier Material materials with Velocidad de flujo del volumen derretido of 0.5 cm³/10min

    ISO 1133

    dry

    230°C/5kg

    Technological properties

    Property
    Application areas

    Fuel Management - Fuel Lines,Fuel Management - In-Tank and Fuel Venting Lines,Chemical Process Industry,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes,Tubing and Hoses,Automotive Cables,Performance Wire,PVDF Cable Jacketing,Wire and Cables,Offshore Umbilicals,Underground Fuel Containment

    Processing methods

    Compression Molding:

  • Molding temperature (°C) ISO 293: 225
  • Molding time (min) ISO 293: 3
  • DeMolding temperature (°C) ISO 293: 120