Constante dieléctrica: 11 [-]

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar® 740

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 740 RED

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2800-00

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2800-20

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2750-01

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Superflex® 2500-20

Suministrada por:

Arkema: High Performance Polymers

Polyamide 46 (PA46)

Stanyl® HFX61S

Suministrada por:

DSM Engineering Materials

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2950-05

Suministrada por:

Arkema: High Performance Polymers

Polyamide 66 (PA66)

Akulon® S223-G6-FC BK00001

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® S223-G6-FC NA99001

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® S223-G6

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® S223-HPG5

Suministrada por:

DSM Engineering Materials

Polyvinylidenefluoride (PVDF)

Kynar Superflex® 2500-25

Suministrada por:

Arkema: High Performance Polymers

Óxido de aluminio

Rubalit® 708S C

Suministrada por:

CeramTec GmbH

Óxido de aluminio

Rubalit® 710F C

Suministrada por:

CeramTec GmbH

Óxido de aluminio

Rubalit® 708HP C

Suministrada por:

CeramTec GmbH

Óxido de aluminio

Rubalit® 708 D

Suministrada por:

CeramTec GmbH