Description

Silicon Nitride (Si₃N₄) is 60% lighter than steel but strong enough to survive some of the most demanding applications in a variety of industries. This lightweight, high-strength ceramic material is used as an alternative to stainless steel, super alloys, tungsten carbides and first-generation ceramics such as Al₂O₃ and ZrO₂. It offers excellent thermal shock resistance and high fracture toughness, compatibility with nonferrous metal melts, and improved structural reliability compared to other ceramic materials.

Los datos sobre este material han sido proporcionados por Innovacera.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

23.0 °C

3.21 g/cm³

Show Supplier Material materials with Densidad of 3.21 g/cm³

Mecánica

PropertyTemperatureValue

Coeficiente de Poisson

23.0 °C

0.25 [-]

Show Supplier Material materials with Coeficiente de Poisson of 0.25 [-]

Dureza Vickers

23.0 °C

1417 [-]

Show Supplier Material materials with Dureza Vickers of 1417 [-]

Módulo elástico

23.0 °C

330 GPa

Show Supplier Material materials with Módulo elástico of 330 GPa

Plane-Strain Fracture Toughnes

23.0 °C

6 - 7 MPa·√m

Show Supplier Material materials with Plane-Strain Fracture Toughnes of 6 - 7 MPa·√m

Resistencia a la flexión

23.0 °C

610 MPa

Show Supplier Material materials with Resistencia a la flexión of 610 MPa

Aplicaciones térmicas

PropertyTemperatureValue

Calor específico

23.0 °C

660 J/(kg·K)

Show Supplier Material materials with Calor específico of 660 J/(kg·K)

Coeficiente de dilatación térmica

23.0 °C

3E-6 - 3.2E-6 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica of 3E-6 - 3.2E-6 1/K

Conductividad térmica

23.0 °C

15 - 20 W/(m·K)

Show Supplier Material materials with Conductividad térmica of 15 - 20 W/(m·K)

Parámetro de choque térmico (R2)

550 W/m

Show Supplier Material materials with Parámetro de choque térmico (R2) of 550 W/m

Eléctrico

PropertyTemperatureValue

Resistividad eléctrica

23.0 °C

1.00E+16 Ω·m

Show Supplier Material materials with Resistividad eléctrica of 1.00E+16 Ω·m

Rigidez dieléctrica

23.0 °C

13 kV/mm

Show Supplier Material materials with Rigidez dieléctrica of 13 kV/mm

Technological properties

Property
Application areas

High precision silicon nitride ceramic balls, roller for bearing, pump valve, Thermocouple Protection Sheaths, Electric heating element, Weld Location Pins

Processing methods

Gas Press Sintering, Cold Isostatic Press, Dry Press, Precision Machining Processing