General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.02 g/cm³ Show Supplier Material materials with Densidad of 1.02 g/cm³ | ISO1183 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dureza Shore D | 23.0 °C | 82 [-] Show Supplier Material materials with Dureza Shore D of 82 [-] | ISO868 | ||
Elongación | 23.0 °C | 50 % Show Supplier Material materials with Elongación of 50 % | ISO527 | ||
Hardness, Ball Indentation | 23.0 °C | 90 MPa Show Supplier Material materials with Hardness, Ball Indentation of 90 MPa | ISO2039-1 | ||
Módulo de flexión | 23.0 °C | 1.6 GPa Show Supplier Material materials with Módulo de flexión of 1.6 GPa | ISO178 | ||
Módulo elástico | 23.0 °C | 1.6 GPa Show Supplier Material materials with Módulo elástico of 1.6 GPa | ISO527 | ||
Resistencia a la flexión | 23.0 °C | 65 MPa Show Supplier Material materials with Resistencia a la flexión of 65 MPa | ISO178 | ||
Resistencia a la tracción | 23.0 °C | 60 MPa Show Supplier Material materials with Resistencia a la tracción of 60 MPa | ISO527 | ||
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | ISO179 | ||
23.0 °C | 14 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14 kJ/m² | ISO179 | |||
Resistencia al choque, ensayo Charpy no entallado | No break @-30, 23°C |
Aplicaciones térmicas
Technological properties
Property | ||
---|---|---|
Application areas | Memory glasses frame, headphones, cosmetic; Electronic connector, infrared sensor cover, mobile, phone shell; Oil cup, clasp, handle, flowmeter, observing Mirror/Window, Oil nozzle cover, milker; Sanitary ware: bracket, water pipe/pressure regulating valve, water filter, window, flowmeter; Food containers: drinking cups, transparent containers, transparent tableware; Motion device: diving device shield, knife handle, waterproof watch case; Medical devices: Protective mask mirror, hearing aid/earphone/ear hang, respiratory mask | |
Processing methods | Drying Temperature: 90-100°C, Drying Time: 6-8 hr, Rear Temperature: 200°C, Middle Temperature: 240°C, Front Temperature: 250°C, Nozzle Temperature: 240°C, Mold Temperature: 60-90°C, Injection Pressure: 80-100 MPa |