General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 11.8 g/cm³ Show Supplier Material materials with Densidad of 11.8 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 260 - 340 [-] Show Supplier Material materials with Dureza Vickers of 260 - 340 [-] |
Elongación | 23.0 °C | 2 - 10 % Show Supplier Material materials with Elongación of 2 - 10 % |
Módulo de cizallamiento | 23.0 °C | 40 GPa Show Supplier Material materials with Módulo de cizallamiento of 40 GPa |
Módulo elástico | 23.0 °C | 108 GPa Show Supplier Material materials with Módulo elástico of 108 GPa |
Resistencia a la tracción | 23.0 °C | 850 - 1150 MPa Show Supplier Material materials with Resistencia a la tracción of 850 - 1150 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.46E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.46E-5 1/K | RT-100 °C |
Conductividad térmica | 23.0 °C | 28 W/(m·K) Show Supplier Material materials with Conductividad térmica of 28 W/(m·K) | |
Temperatura de fusión | 1130 - 1180 °C Show Supplier Material materials with Temperatura de fusión of 1130 - 1180 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Coeficiente de temperatura de la resistencia | 23.0 °C | 2.8E-4 1/K Show Supplier Material materials with Coeficiente de temperatura de la resistencia of 2.8E-4 1/K |
Resistividad eléctrica | 23.0 °C | 3.38E-7 - 3.59E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3.38E-7 - 3.59E-7 Ω·m |
Specific Electrical conductivity | 4.8 - 5.1 % IACS Show Supplier Material materials with Specific Electrical conductivity of 4.8 - 5.1 % IACS |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding contacts, Slip ring brushes, Potentiometers, probe pins | |
Corrosion properties | Corrosion resistant | |
Other | Superb sliding contact alloy, stable contact resistance, wear resistant, Oxidation resistant up to 300 °C, Ductile |