General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 14.3 g/cm³ Show Supplier Material materials with Densidad of 14.3 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 120 - 220 [-] Show Supplier Material materials with Dureza Vickers of 120 - 220 [-] | |
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % | min. |
Módulo de cizallamiento | 23.0 °C | 44 GPa Show Supplier Material materials with Módulo de cizallamiento of 44 GPa | |
Módulo elástico | 23.0 °C | 124 GPa Show Supplier Material materials with Módulo elástico of 124 GPa | |
Resistencia a la tracción | 23.0 °C | 500 - 750 MPa Show Supplier Material materials with Resistencia a la tracción of 500 - 750 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.41E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.41E-5 1/K | RT-100 °C |
Conductividad térmica | 23.0 °C | 31 W/(m·K) Show Supplier Material materials with Conductividad térmica of 31 W/(m·K) | |
Temperatura de fusión | 1190 - 1230 °C Show Supplier Material materials with Temperatura de fusión of 1190 - 1230 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Coeficiente de temperatura de la resistencia | 23.0 °C | 1.8E-4 1/K Show Supplier Material materials with Coeficiente de temperatura de la resistencia of 1.8E-4 1/K |
Resistividad eléctrica | 23.0 °C | 2.87E-7 - 3.13E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2.87E-7 - 3.13E-7 Ω·m |
Specific Electrical conductivity | 5.5 - 6 % IACS Show Supplier Material materials with Specific Electrical conductivity of 5.5 - 6 % IACS |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding contacts, Slip ring brushes | |
Corrosion properties | Corrosion resistant | |
Other | Oxidation resistant, Ductile, Age hardenable, Wear Resistant, stable contact resistant |