General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 15.1 g/cm³ Show Supplier Material materials with Densidad of 15.1 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 220 - 300 [-] Show Supplier Material materials with Dureza Vickers of 220 - 300 [-] |
Elongación | 23.0 °C | 3 - 15 % Show Supplier Material materials with Elongación of 3 - 15 % |
Módulo de cizallamiento | 23.0 °C | 37 GPa Show Supplier Material materials with Módulo de cizallamiento of 37 GPa |
Módulo elástico | 23.0 °C | 87 GPa Show Supplier Material materials with Módulo elástico of 87 GPa |
Resistencia a la tracción | 23.0 °C | 650 - 900 MPa Show Supplier Material materials with Resistencia a la tracción of 650 - 900 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.67E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.67E-5 1/K | RT-100 °C |
Conductividad térmica | 23.0 °C | 66 W/(m·K) Show Supplier Material materials with Conductividad térmica of 66 W/(m·K) | |
Temperatura de fusión | 865 - 895 °C Show Supplier Material materials with Temperatura de fusión of 865 - 895 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Coeficiente de temperatura de la resistencia | 23.0 °C | 5.2E-4 1/K Show Supplier Material materials with Coeficiente de temperatura de la resistencia of 5.2E-4 1/K |
Resistividad eléctrica | 23.0 °C | 1.25E-7 - 1.45E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.25E-7 - 1.45E-7 Ω·m |
Specific Electrical conductivity | 11.9 - 13.8 % IACS Show Supplier Material materials with Specific Electrical conductivity of 11.9 - 13.8 % IACS |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding contacts, Slip ring brushes, Resistance wires | |
Corrosion properties | Corrosion resistant | |
Other | Wear resistant, Age hardenable, Ductile, High electrical conductivity, Stable Contact resistant |