General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 10.13 g/cm³ Show Supplier Material materials with Densidad of 10.13 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 80 - 120 [-] Show Supplier Material materials with Dureza Vickers of 80 - 120 [-] | |
Elongación | 23.0 °C | 20 % Show Supplier Material materials with Elongación of 20 % | min. |
Límite elástico Rp 0,2 | 23.0 °C | 200 - 300 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 200 - 300 MPa | |
Módulo elástico | 23.0 °C | 85 GPa Show Supplier Material materials with Módulo elástico of 85 GPa | |
Resistencia a la tracción | 23.0 °C | 300 - 400 MPa Show Supplier Material materials with Resistencia a la tracción of 300 - 400 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.93E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.93E-5 1/K | RT-100 °C |
Temperatura de fusión | 779 - 820 °C Show Supplier Material materials with Temperatura de fusión of 779 - 820 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Coeficiente de temperatura de la resistencia | 23.0 °C | 4.3E-4 1/K Show Supplier Material materials with Coeficiente de temperatura de la resistencia of 4.3E-4 1/K |
Resistividad eléctrica | 23.0 °C | 2.2E-8 - 2.5E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2.2E-8 - 2.5E-8 Ω·m |
Specific Electrical conductivity | 70 - 77 % IACS Show Supplier Material materials with Specific Electrical conductivity of 70 - 77 % IACS |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding contacts, Slip ring brushes, switching contacts | |
Corrosion properties | Corrosion resistant | |
Other | Ductile, High conductivity, Low contact resistance, Susceptible to attack by sulphur |