General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 21.54 g/cm³ Show Supplier Material materials with Densidad of 21.54 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 100 - 130 [-] Show Supplier Material materials with Dureza Vickers of 100 - 130 [-] | |
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % | min. |
Límite elástico Rp 0,2 | 23.0 °C | 200 - 370 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 200 - 370 MPa | |
Módulo de cizallamiento | 23.0 °C | 72 GPa Show Supplier Material materials with Módulo de cizallamiento of 72 GPa | |
Módulo elástico | 23.0 °C | 215 GPa Show Supplier Material materials with Módulo elástico of 215 GPa | |
Resistencia a la tracción | 23.0 °C | 320 - 450 MPa Show Supplier Material materials with Resistencia a la tracción of 320 - 450 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.7E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.7E-6 1/K | up to 300°C |
Temperatura de fusión | 1780 - 1800 °C Show Supplier Material materials with Temperatura de fusión of 1780 - 1800 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de temperatura de la resistencia | 23.0 °C | 1.21E-3 - 1.26E-3 1/K Show Supplier Material materials with Coeficiente de temperatura de la resistencia of 1.21E-3 - 1.26E-3 1/K | 0-100 °C |
Resistividad eléctrica | 23.0 °C | 2.45E-7 - 2.52E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2.45E-7 - 2.52E-7 Ω·m | |
Specific Electrical conductivity | 6.8 - 7.02 % IACS Show Supplier Material materials with Specific Electrical conductivity of 6.8 - 7.02 % IACS |
Technological properties
Property | ||
---|---|---|
Application areas | Spark plugs, electrodes, thermocouples | |
Corrosion properties | Corrosion resistant | |
Other | Ductile, Biocompatible |