General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 21.36 g/cm³ Show Supplier Material materials with Densidad of 21.36 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 73 [-] Show Supplier Material materials with Dureza Vickers of 73 [-] | |
Elongación | 1200.0 °C | 52 % Show Supplier Material materials with Elongación of 52 % | |
1400.0 °C | 48 % Show Supplier Material materials with Elongación of 48 % | ||
Límite elástico Rp 0,2 | 1200.0 °C | 19 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 19 MPa | |
1400.0 °C | 15 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 15 MPa | ||
Resistencia a la fluencia | 1200.0 °C | 12 MPa Show Supplier Material materials with Resistencia a la fluencia of 12 MPa | 10,000 h (extrapolated data) |
1400.0 °C | 4.3 MPa Show Supplier Material materials with Resistencia a la fluencia of 4.3 MPa | 10,000 h (extrapolated data) | |
Resistencia a la tracción | 1200.0 °C | 24 MPa Show Supplier Material materials with Resistencia a la tracción of 24 MPa | |
1400.0 °C | 16 MPa Show Supplier Material materials with Resistencia a la tracción of 16 MPa | ||
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 20.0 °C | 71.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 71.5 W/(m·K) |
1200.0 °C | 84.2 W/(m·K) Show Supplier Material materials with Conductividad térmica of 84.2 W/(m·K) | |
1400.0 °C | 85 W/(m·K) Show Supplier Material materials with Conductividad térmica of 85 W/(m·K) | |
Temperatura de fusión | 1769 °C Show Supplier Material materials with Temperatura de fusión of 1769 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 1.2E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.2E-7 Ω·m |
1200.0 °C | 5.4E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.4E-7 Ω·m | |
1400.0 °C | 5.9E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.9E-7 Ω·m | |