General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 20.73 g/cm³ Show Supplier Material materials with Densidad of 20.73 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 73 [-] Show Supplier Material materials with Dureza Vickers of 73 [-] |
Elongación | 20.0 °C | 32.6 % Show Supplier Material materials with Elongación of 32.6 % |
1200.0 °C | 57 % Show Supplier Material materials with Elongación of 57 % | |
1400.0 °C | 63 % Show Supplier Material materials with Elongación of 63 % | |
1600.0 °C | 55 % Show Supplier Material materials with Elongación of 55 % | |
Límite elástico Rp 0,2 | 20.0 °C | 114 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 114 MPa |
1200.0 °C | 27.1 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 27.1 MPa | |
1400.0 °C | 17.8 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 17.8 MPa | |
1600.0 °C | 10.1 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 10.1 MPa | |
Módulo elástico | 23.0 °C | 97.02 GPa Show Supplier Material materials with Módulo elástico of 97.02 GPa |
Resistencia a la tracción | 20.0 °C | 231 MPa Show Supplier Material materials with Resistencia a la tracción of 231 MPa |
1200.0 °C | 44.2 MPa Show Supplier Material materials with Resistencia a la tracción of 44.2 MPa | |
1400.0 °C | 25.3 MPa Show Supplier Material materials with Resistencia a la tracción of 25.3 MPa | |
1600.0 °C | 13.2 MPa Show Supplier Material materials with Resistencia a la tracción of 13.2 MPa | |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 20.0 °C | 45.74 W/(m·K) Show Supplier Material materials with Conductividad térmica of 45.74 W/(m·K) |
1200.0 °C | 75.9 W/(m·K) Show Supplier Material materials with Conductividad térmica of 75.9 W/(m·K) | |
1400.0 °C | 77.16 W/(m·K) Show Supplier Material materials with Conductividad térmica of 77.16 W/(m·K) | |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 1.7E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.7E-7 Ω·m |
1146.0 °C | 5.2E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.2E-7 Ω·m | |