General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 20 g/cm³ Show Supplier Material materials with Densidad of 20 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 113 [-] Show Supplier Material materials with Dureza Vickers of 113 [-] | |
Elongación | 20.0 °C | 27 % Show Supplier Material materials with Elongación of 27 % | |
1200.0 °C | 34 % Show Supplier Material materials with Elongación of 34 % | ||
1400.0 °C | 69 % Show Supplier Material materials with Elongación of 69 % | ||
1600.0 °C | 66 % Show Supplier Material materials with Elongación of 66 % | ||
Límite elástico Rp 0,2 | 20.0 °C | 211 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 211 MPa | |
1200.0 °C | 51.3 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 51.3 MPa | ||
1400.0 °C | 34.8 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 34.8 MPa | ||
1600.0 °C | 22 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 22 MPa | ||
Módulo elástico | 23.0 °C | 162 GPa Show Supplier Material materials with Módulo elástico of 162 GPa | |
Norton Exponent | 1200.0 °C | 7 [-] Show Supplier Material materials with Norton Exponent of 7 [-] | |
1400.0 °C | 6.1 [-] Show Supplier Material materials with Norton Exponent of 6.1 [-] | ||
1600.0 °C | 6.2 [-] Show Supplier Material materials with Norton Exponent of 6.2 [-] | ||
Resistencia a la fluencia | 1200.0 °C | 5.6 MPa Show Supplier Material materials with Resistencia a la fluencia of 5.6 MPa | 10,000 h (extrapolated data) |
1400.0 °C | 3.3 MPa Show Supplier Material materials with Resistencia a la fluencia of 3.3 MPa | 10,000 h (extrapolated data) | |
1600.0 °C | 1.8 MPa Show Supplier Material materials with Resistencia a la fluencia of 1.8 MPa | 10,000 h (extrapolated data) | |
Resistencia a la tracción | 20.0 °C | 371 MPa Show Supplier Material materials with Resistencia a la tracción of 371 MPa | |
1200.0 °C | 62.8 MPa Show Supplier Material materials with Resistencia a la tracción of 62.8 MPa | ||
1400.0 °C | 36.6 MPa Show Supplier Material materials with Resistencia a la tracción of 36.6 MPa | ||
1600.0 °C | 22.2 MPa Show Supplier Material materials with Resistencia a la tracción of 22.2 MPa | ||
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 20.0 °C | 40 W/(m·K) Show Supplier Material materials with Conductividad térmica of 40 W/(m·K) |
1200.0 °C | 66.7 W/(m·K) Show Supplier Material materials with Conductividad térmica of 66.7 W/(m·K) | |
1400.0 °C | 69.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 69.5 W/(m·K) | |
Temperatura de fusión | 1840 - 1870 °C Show Supplier Material materials with Temperatura de fusión of 1840 - 1870 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 2E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2E-7 Ω·m |
1156.0 °C | 5.5E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.5E-7 Ω·m | |
1400.0 °C | 6.1E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 6.1E-7 Ω·m | |
Technological properties
Property | ||
---|---|---|
Application areas | Pt-10%Rh DPH is very widely used for structural applications in the glass industry. Typical uses are in the manufacture of feeder systems, stirrers, thermocouple thimbles, bubbler tubes, linings for refractory components and in glass fiber bushings. |