General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 3.7 g/cm³ Show Supplier Material materials with Densidad of 3.7 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.22 - 0.23 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.22 - 0.23 [-] |
Dureza Vickers | 23.0 °C | 1377 [-] Show Supplier Material materials with Dureza Vickers of 1377 [-] |
Módulo elástico | 23.0 °C | 280 - 320 GPa Show Supplier Material materials with Módulo elástico of 280 - 320 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 4 - 5 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4 - 5 MPa·√m |
Resistencia a la compresión | 23.0 °C | 2068 MPa Show Supplier Material materials with Resistencia a la compresión of 2068 MPa |
Resistencia a la flexión | 23.0 °C | 323.7 MPa Show Supplier Material materials with Resistencia a la flexión of 323.7 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 780 J/(kg·K) Show Supplier Material materials with Calor específico of 780 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 8.2E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8.2E-6 1/K |
Conductividad térmica | 23.0 °C | 23 W/(m·K) Show Supplier Material materials with Conductividad térmica of 23 W/(m·K) |
Parámetro de choque térmico (R2) | 200 W/m Show Supplier Material materials with Parámetro de choque térmico (R2) of 200 W/m |
Eléctrico
Property | Temperature | Value |
---|---|---|
Constante dieléctrica | 23.0 °C | 9 [-] Show Supplier Material materials with Constante dieléctrica of 9 [-] |
Resistividad eléctrica | 23.0 °C | 1.00E+16 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.00E+16 Ω·m |
Rigidez dieléctrica | 23.0 °C | 15 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 15 kV/mm |
Tangente de pérdidas | 23.0 °C | 4E-4 [-] Show Supplier Material materials with Tangente de pérdidas of 4E-4 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Wear ceramic parts: Ceramic Nozzles, Sprayers Cyclones, Homogenising devices, Ceramic Linings, Milling Systems, Ceramic Thread guides - Precision components: Ceramic Measuring Components, Ceramic Control systems, (Micro) dosing valves, Electronic Components, Mechatronics, Optical applications - Machine-construction: Positioning Guide parts, Coatings, Transport ceramic rollers, Ceramic Dies, Textile machine parts, Furnace parts - Rotating equipment: Ceramic Sliding Bearings, Ceramic Ball bearings, Mechanical seals, Ceramic Plungers, Ceramic Valves / fittings, Dosing components - Cutting & moulding: Ceramic knives, Metal-forming tools, Seaming rolls, Ceramic Punches, Drawing dies | |
Processing methods | Ceramic Injection Molding, Low Pressure Injection Molding, Cold Isostatic Press, Dry Press, Precision Machining Processing |