General
Property | Value | Comment |
---|---|---|
Absorción de agua | 0.01 % Show Supplier Material materials with Absorción de agua of 0.01 % | ISO 62 |
Densidad | 0.91 g/cm³ Show Supplier Material materials with Densidad of 0.91 g/cm³ | ISO 1183 |
Mecánica
Property | Value | Comment | |
---|---|---|---|
Dureza Shore D | 70 [-] Show Supplier Material materials with Dureza Shore D of 70 [-] | DIN 53505 | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | min., ISO 527 | |
Elongation at yield | 10 % Show Supplier Material materials with Elongation at yield of 10 % | ISO 527 | |
Hardness, Ball Indentation | 67 MPa Show Supplier Material materials with Hardness, Ball Indentation of 67 MPa | ISO 2039-1 | |
Límite elástico | 30 MPa Show Supplier Material materials with Límite elástico of 30 MPa | ISO 527 | |
Módulo elástico | 1 GPa Show Supplier Material materials with Módulo elástico of 1 GPa | ISO 527 | |
Resistencia al choque, ensayo Charpy entallado | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 50 kJ/m² | ISO 179 | |
Resistencia al choque, ensayo Charpy no entallado | No break, ISO 179 |
Aplicaciones térmicas
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 96 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 96 °C | 0.45 MPa | |||
Temperatura de reblandecimiento Vicat | 91 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 91 °C | ISO 306, VST B50 | |||
Temperatura máx. de funcionamiento | 100 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 100 °C | Longterm | |||
Long | |||||
Short | |||||
Temperatura mín. de funcionamiento | 5 °C Show Supplier Material materials with Temperatura mín. de funcionamiento of 5 °C | Longterm | |||
Inflamabilidad | HB UL 94 |
Eléctrico
Property | Value | Comment |
---|---|---|
Constante dieléctrica | 2.3 [-] Show Supplier Material materials with Constante dieléctrica of 2.3 [-] | DIN 53483 |
Tangente de pérdidas | 0.0002 [-] Show Supplier Material materials with Tangente de pérdidas of 0.0002 [-] | DIN 53483 |
Volume resistivity | 1e+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+16 Ω·cm | min., VDE 0303 |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS,REACH | |
UV resistance | Partly |