General
Property | Value | Comment |
---|---|---|
Absorción de agua | 0.2 % Show Supplier Material materials with Absorción de agua of 0.2 % | ISO 62 |
Coefficient of friction | 0.3 [-] Show Supplier Material materials with Coefficient of friction of 0.3 [-] | DIN 53375, C, Against dry running steel |
Densidad | 1.39 g/cm³ Show Supplier Material materials with Densidad of 1.39 g/cm³ | ISO 1183 |
Mecánica
Property | Value | Comment | |
---|---|---|---|
Dureza Shore D | 83 [-] Show Supplier Material materials with Dureza Shore D of 83 [-] | DIN 53505 | |
Elongación | 31 % Show Supplier Material materials with Elongación of 31 % | ISO 527 | |
Elongation at yield | 10 % Show Supplier Material materials with Elongation at yield of 10 % | ISO 527 | |
Hardness, Ball Indentation | 125 MPa Show Supplier Material materials with Hardness, Ball Indentation of 125 MPa | ISO 2039-1 | |
Límite elástico | 63 MPa Show Supplier Material materials with Límite elástico of 63 MPa | ISO 527 | |
Módulo elástico | 3 GPa Show Supplier Material materials with Módulo elástico of 3 GPa | ISO 527 | |
Resistencia al choque, ensayo Charpy entallado | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | ISO 179 | |
Resistencia al choque, ensayo Charpy no entallado | No break, ISO 179 |
Aplicaciones térmicas
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 0.00012 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.00012 1/K | DIN 53752 | |||
Conductividad térmica | 0.31 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.31 W/(m·K) | EN 52612 | |||
Temperatura de flexión bajo carga | 95 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 95 °C | 2 MPa | |||
Temperatura de reblandecimiento Vicat | 150 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 150 °C | ISO 306, VST B50 | |||
Temperatura máx. de funcionamiento | 100 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 100 °C | Longterm | |||
Long | |||||
Short | |||||
Inflamabilidad | HB UL 94 |
Eléctrico
Property | Value | Comment |
---|---|---|
Constante dieléctrica | 3.8 [-] Show Supplier Material materials with Constante dieléctrica of 3.8 [-] | DIN 53483 |
Rigidez dieléctrica | 40 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 40 kV/mm | VDE 0303 |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | min., VDE 0303 |
Tangente de pérdidas | 0.005 [-] Show Supplier Material materials with Tangente de pérdidas of 0.005 [-] | DIN 53483 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | min., VDE 0303 |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | IEC 60112 |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical engineering, gear wheels, rollers and snap fits | |
Certifications | Food Contact: FDA and EU 10/2011, RoHS,REACH |