General
Property | Value | Comment |
---|---|---|
Absorción de agua | 0.25 % Show Supplier Material materials with Absorción de agua of 0.25 % | ISO 62 |
Coefficient of friction | 0.3 [-] Show Supplier Material materials with Coefficient of friction of 0.3 [-] | DIN 53375, C, Against dry running steel |
Densidad | 1.39 g/cm³ Show Supplier Material materials with Densidad of 1.39 g/cm³ | ISO 1183 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore D | 84 [-] Show Supplier Material materials with Dureza Shore D of 84 [-] | DIN 53505 |
Elongación | 15 % Show Supplier Material materials with Elongación of 15 % | ISO 527 |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | ISO 527 |
Hardness, Ball Indentation | 170 MPa Show Supplier Material materials with Hardness, Ball Indentation of 170 MPa | ISO 2039-1 |
Hardness, Rockwell R | 96 [-] Show Supplier Material materials with Hardness, Rockwell R of 96 [-] | ISO 2039-1 |
Límite elástico | 90 MPa Show Supplier Material materials with Límite elástico of 90 MPa | ISO 527 |
Módulo elástico | 4 GPa Show Supplier Material materials with Módulo elástico of 4 GPa | ISO 527 |
Resistencia al choque, ensayo Charpy entallado | 2 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2 kJ/m² | ISO 179 |
Resistencia al choque, ensayo Charpy no entallado | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | min., ISO 179 |
Aplicaciones térmicas
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 8e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8e-05 1/K | DIN 53752 | |||
Conductividad térmica | 0.29 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.29 W/(m·K) | DIN 52612 | |||
Temperatura de flexión bajo carga | 80 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 80 °C | 2 MPa | |||
Temperatura máx. de funcionamiento | 100 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 100 °C | Longterm | |||
Long | |||||
Short | |||||
Temperatura mín. de funcionamiento | -20 °C Show Supplier Material materials with Temperatura mín. de funcionamiento of -20 °C | Longterm | |||
Inflamabilidad | HB UL 94 |
Eléctrico
Property | Value | Comment |
---|---|---|
Constante dieléctrica | 3.2 [-] Show Supplier Material materials with Constante dieléctrica of 3.2 [-] | DIN 53483 |
Rigidez dieléctrica | 22 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 22 kV/mm | VDE 0303 |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | min., VDE 0303 |
Tangente de pérdidas | 0.014 [-] Show Supplier Material materials with Tangente de pérdidas of 0.014 [-] | DIN 53483 |
Volume resistivity | 1e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm | min., VDE 0303 |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | IEC 60112 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts and rollers | |
Certifications | RoHS,REACH |