General
Property | Value | Comment |
---|---|---|
Absorción de agua | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | ISO 62 |
Coefficient of friction | 0.2 [-] Show Supplier Material materials with Coefficient of friction of 0.2 [-] | DIN 53375, B, Against dry running steel |
Densidad | 1.32 g/cm³ Show Supplier Material materials with Densidad of 1.32 g/cm³ | ISO 1183 |
Mecánica
Property | Value | Comment | |
---|---|---|---|
Dureza Shore D | 90 [-] Show Supplier Material materials with Dureza Shore D of 90 [-] | DIN 53505 | |
Elongación | 25 % Show Supplier Material materials with Elongación of 25 % | ISO 527 | |
Hardness, Rockwell R | 99 [-] Show Supplier Material materials with Hardness, Rockwell R of 99 [-] | ISO 2039-1 | |
Límite elástico | 95 MPa Show Supplier Material materials with Límite elástico of 95 MPa | ISO 527 | |
Módulo elástico | 3 GPa Show Supplier Material materials with Módulo elástico of 3 GPa | ISO 527 | |
Resistencia a la flexión | 170 MPa Show Supplier Material materials with Resistencia a la flexión of 170 MPa | ISO 178 | |
Resistencia al choque, ensayo Charpy entallado | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | ISO 179 | |
Resistencia al choque, ensayo Charpy no entallado | No break, ISO 179 |
Aplicaciones térmicas
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 5e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5e-05 1/K | DIN 53752 | |||
Conductividad térmica | 0.25 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.25 W/(m·K) | DIN 52612 | |||
Temperatura de flexión bajo carga | 140 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 140 °C | 2 MPa | |||
182 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 182 °C | 0.45 MPa | ||||
Temperatura de reblandecimiento Vicat | 250 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 250 °C | ISO 306, VST B50 | |||
Temperatura máx. de funcionamiento | 260 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 260 °C | Longterm | |||
Long | |||||
Short | |||||
Temperatura mín. de funcionamiento | -40 °C Show Supplier Material materials with Temperatura mín. de funcionamiento of -40 °C | Longterm | |||
Inflamabilidad | V-0 UL 94 |
Eléctrico
Property | Value | Comment |
---|---|---|
Constante dieléctrica | 3.2 [-] Show Supplier Material materials with Constante dieléctrica of 3.2 [-] | DIN 53483 |
Rigidez dieléctrica | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | VDE 0303 |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | min., VDE 0303 |
Tangente de pérdidas | 0.003 [-] Show Supplier Material materials with Tangente de pérdidas of 0.003 [-] | DIN 53483 |
Volume resistivity | 1e+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+16 Ω·cm | min., VDE 0303 |
Índice de seguimiento comparativo | 150 V Show Supplier Material materials with Índice de seguimiento comparativo of 150 V | IEC 60112 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts, blindings and for applications at very high temperatures | |
Certifications | Food Contact: FDA and EU 10/2011, RoHS,REACH | |
UV resistance | Partly |