General
Property | Value | Comment |
---|---|---|
Absorción de agua | 0.01 % Show Supplier Material materials with Absorción de agua of 0.01 % | ISO 62 |
Coefficient of friction | 0.12 [-] Show Supplier Material materials with Coefficient of friction of 0.12 [-] | DIN 53375, A, Against dry running steel |
Densidad | 0.93 g/cm³ Show Supplier Material materials with Densidad of 0.93 g/cm³ | ISO 1183 |
Mecánica
Property | Value | Comment | |
---|---|---|---|
Dureza Shore D | 63 [-] Show Supplier Material materials with Dureza Shore D of 63 [-] | DIN 53505 | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | min., ISO 527 | |
Elongation at yield | 8 % Show Supplier Material materials with Elongation at yield of 8 % | min., ISO 527 | |
Hardness, Ball Indentation | 38 MPa Show Supplier Material materials with Hardness, Ball Indentation of 38 MPa | ISO 2039-1 | |
Límite elástico | 17 MPa Show Supplier Material materials with Límite elástico of 17 MPa | ISO 527 | |
Módulo elástico | 0.7 GPa Show Supplier Material materials with Módulo elástico of 0.7 GPa | min., ISO 527 | |
Resistencia a desgarros | 40 kN/m Show Supplier Material materials with Resistencia a desgarros of 40 kN/m | min., ISO 527 | |
Resistencia a la flexión | 27 MPa Show Supplier Material materials with Resistencia a la flexión of 27 MPa | ISO 178 | |
Resistencia al choque, ensayo Charpy entallado | No break, ISO 179 | ||
Resistencia al choque, ensayo Charpy no entallado | No break, ISO 179 |
Aplicaciones térmicas
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 0.0002 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.0002 1/K | DIN 53752 | |||
Conductividad térmica | 0.41 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.41 W/(m·K) | DIN 52612 | |||
Temperatura de flexión bajo carga | 42 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 42 °C | 2 MPa | |||
65 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 65 °C | 0.45 MPa | ||||
Temperatura de reblandecimiento Vicat | 79 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 79 °C | ISO 306, VST B50 | |||
Temperatura máx. de funcionamiento | 90 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 90 °C | Longterm | |||
Long | |||||
Short | |||||
Temperatura mín. de funcionamiento | -150 °C Show Supplier Material materials with Temperatura mín. de funcionamiento of -150 °C | Longterm | |||
Inflamabilidad | HB UL 94 |
Eléctrico
Property | Value | Comment |
---|---|---|
Constante dieléctrica | 3 [-] Show Supplier Material materials with Constante dieléctrica of 3 [-] | DIN 53483 |
Rigidez dieléctrica | 45 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 45 kV/mm | VDE 0303 |
Surface resistivity | 1e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+11 Ω/sq | min., VDE 0303 |
Tangente de pérdidas | 0.0001 [-] Show Supplier Material materials with Tangente de pérdidas of 0.0001 [-] | DIN 53483 |
Volume resistivity | 1e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm | min., VDE 0303 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts, chain guidance and sliding profiles | |
Certifications | Food Contact: FDA and EU 10/2011, RoHS,REACH |