General
Property | Value | Comment |
---|---|---|
Absorción de agua | 0.01 % Show Supplier Material materials with Absorción de agua of 0.01 % | ISO 62 |
Coefficient of friction | 0.08 [-] Show Supplier Material materials with Coefficient of friction of 0.08 [-] | DIN 53375, A, Against dry running steel |
Densidad | 0.93 g/cm³ Show Supplier Material materials with Densidad of 0.93 g/cm³ | ISO 1183 |
Mecánica
Property | Value | Comment | |
---|---|---|---|
Dureza Shore D | 61 [-] Show Supplier Material materials with Dureza Shore D of 61 [-] | DIN 53505 | |
Elongation at yield | 20 % Show Supplier Material materials with Elongation at yield of 20 % | ISO 527 | |
Hardness, Ball Indentation | 35 MPa Show Supplier Material materials with Hardness, Ball Indentation of 35 MPa | ||
Límite elástico | 17 MPa Show Supplier Material materials with Límite elástico of 17 MPa | ISO 527 | |
Módulo elástico | 0.68 GPa Show Supplier Material materials with Módulo elástico of 0.68 GPa | min., ISO 527 | |
Resistencia a la flexión | 27 MPa Show Supplier Material materials with Resistencia a la flexión of 27 MPa | ISO 178 | |
Resistencia a la tracción | 28 MPa Show Supplier Material materials with Resistencia a la tracción of 28 MPa | DIN 53455 | |
Elongación | No break, ISO 527 | ||
Resistencia a desgarros | No break, ISO 527 | ||
Resistencia al choque, ensayo Charpy entallado | No break, ISO 179 | ||
Resistencia al choque, ensayo Charpy no entallado | No break, ISO 179 |
Aplicaciones térmicas
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 0.0002 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.0002 1/K | DIN 53752 | |||
Conductividad térmica | 0.41 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.41 W/(m·K) | DIN 52612 | |||
Temperatura de flexión bajo carga | 42 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 42 °C | 0.45 MPa | |||
Temperatura de reblandecimiento Vicat | 80 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 80 °C | ISO 306, VST B50 | |||
Temperatura máx. de funcionamiento | 80 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 80 °C | Longterm | |||
Long | |||||
Short | |||||
Temperatura mín. de funcionamiento | -150 °C Show Supplier Material materials with Temperatura mín. de funcionamiento of -150 °C | Longterm | |||
Inflamabilidad | HB UL 94 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts, chain guidance and sliding profiles | |
Certifications | Food Contact: FDA and EU 10/2011, RoHS,REACH |