General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.54 - 1.6 g/cm³ Show Supplier Material materials with Densidad of 1.54 - 1.6 g/cm³ | ISO 1183 |
Recycled Content | 25 % Show Supplier Material materials with Recycled Content of 25 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.4 % Show Supplier Material materials with Elongación of 1.4 % | ISO 527, 5 mm/min |
Módulo de flexión | 23.0 °C | 8.5 GPa Show Supplier Material materials with Módulo de flexión of 8.5 GPa | ISO 178, 2 mm/min |
Resistencia a la flexión | 23.0 °C | 140 MPa Show Supplier Material materials with Resistencia a la flexión of 140 MPa | ISO 178, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | ISO 527-2/1A, 10 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 6.4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6.4 kJ/m² | ISO 179eA |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 5.9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 5.9 kJ/m² | min., ISO 180 |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Contenido de cenizas | 23.0 °C | 30 - 35 % Show Supplier Material materials with Contenido de cenizas of 30 - 35 % | ASTM D5630 | ||
Heat deflection temperature, 0.45 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 205 °C | ISO 75 | |||
Temperatura de fusión | 242 °C Show Supplier Material materials with Temperatura de fusión of 242 °C | ISO 3146 | |||
Inflamabilidad | V-0 for 3.2 mm sample UL94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 1kHz | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 2E-3 [-] | ASTM D150 |
Rigidez dieléctrica | 23.0 °C | 32 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 32 kV/mm | ASTM D149, 1.6 mm, 500V/s in oil |
Volume resistivity | 23.0 °C | 1.00E+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm | ASTM D257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 - 0.5 % Show Supplier Material materials with Contracción of 0.2 - 0.5 % | ASTM D955 |
Contracción transversal | 23.0 °C | 0.6 - 0.9 % Show Supplier Material materials with Contracción transversal of 0.6 - 0.9 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical components (e.g. connectros) and structural components. | |
Certifications | RoHS,RECH,ULE Environmental Claims Validation | |
Color | Black | |
Fillers | 30% Glass Fiber and Mineral Powder | |
Processing methods |