General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.68 g/cm³ Show Supplier Material materials with Densidad of 1.68 g/cm³ | ISO 1183 |
Recycled Content | 43 % Show Supplier Material materials with Recycled Content of 43 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo de flexión | 23.0 °C | 10 GPa Show Supplier Material materials with Módulo de flexión of 10 GPa | ISO 178, 2 mm/min |
Resistencia a la flexión | 23.0 °C | 190 MPa Show Supplier Material materials with Resistencia a la flexión of 190 MPa | ISO 178, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 125 MPa Show Supplier Material materials with Resistencia a la tracción of 125 MPa | ISO 527, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 8.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 8.5 kJ/m² | ISO 180 |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Contenido de cenizas | 23.0 °C | 30 % Show Supplier Material materials with Contenido de cenizas of 30 % | ASTM D5630 | ||
Heat deflection temperature, 1.80 MPa | 220 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 220 °C | ISO 75 | |||
Inflamabilidad | V0, V0 5VA for 3.2 mm sample UL94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 29 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 29 kV/mm | ASTM D149, 1.6 mm, 500V/s in oil |
Volume resistivity | 23.0 °C | 1.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm | ASTM D257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electrical components, appliances and structral applications. | |
Certifications | RoHS,RECH,ULE Environmental Claims Validation | |
Color | Black | |
Fillers | 30% Glass Fiber | |
Processing methods |