General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.06 % Show Supplier Material materials with Absorción de agua of 0.06 % | ASTM D570, 23°C/24hr |
Densidad | 23.0 °C | 1.4 g/cm³ Show Supplier Material materials with Densidad of 1.4 g/cm³ | ISO 1183 |
Recycled Content | 35 % Show Supplier Material materials with Recycled Content of 35 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo de flexión | 23.0 °C | 5 GPa Show Supplier Material materials with Módulo de flexión of 5 GPa | ISO 178, 2 mm/min |
Resistencia a la flexión | 23.0 °C | 160 MPa Show Supplier Material materials with Resistencia a la flexión of 160 MPa | ISO 178, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 102 MPa Show Supplier Material materials with Resistencia a la tracción of 102 MPa | ISO 527, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | ISO 179eA |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 40 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | ISO 179eA |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Contenido de cenizas | 23.0 °C | 15 % Show Supplier Material materials with Contenido de cenizas of 15 % | ASTM D5630 | ||
Heat deflection temperature, 1.80 MPa | 186 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 186 °C | ISO-75 | |||
Temperatura de fusión | 240 °C Show Supplier Material materials with Temperatura de fusión of 240 °C | ISO 3146 | |||
Inflamabilidad | HB for 3.2 mm sample UL94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 1kHz | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 2E-3 [-] | ASTM D150 |
Rigidez dieléctrica | 23.0 °C | 32 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 32 kV/mm | ASTM D149, 1.6 mm, 500V/s in oil |
Surface resistivity | 23.0 °C | 1.00E+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+15 Ω/sq | ASTM D257 |
Volume resistivity | 23.0 °C | 8.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 8.00E+16 Ω·cm | ASTM D257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 - 0.5 % Show Supplier Material materials with Contracción of 0.4 - 0.5 % | ASTM D955 |
Contracción transversal | 23.0 °C | 0.5 - 0.8 % Show Supplier Material materials with Contracción transversal of 0.5 - 0.8 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Eelcrtical components (e.g. connectros) and structural components. | |
Certifications | RoHS,RECH,ULE Environmental Claims Validation | |
Fillers | 15% Glass Fiber | |
Processing methods |