General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.33 g/cm³ Show Supplier Material materials with Densidad of 1.33 g/cm³ | ISO 1183 |
Recycled Content | 99 % Show Supplier Material materials with Recycled Content of 99 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Límite elástico | 23.0 °C | 58 MPa Show Supplier Material materials with Límite elástico of 58 MPa | ASTM D638, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.8 GPa Show Supplier Material materials with Módulo de flexión of 2.8 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 90 MPa Show Supplier Material materials with Resistencia a la flexión of 90 MPa | ASTM D790, 1.3 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 33 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 33 kJ/m² | ISO 180 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 72 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 72 °C | ASTM D648 | |
Temperatura de fusión | 246 °C Show Supplier Material materials with Temperatura de fusión of 246 °C | ASTM D3418 | |
Inflamabilidad | HB for 3.2 mm sample UL94 |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS,RECH,ULE Environmental Claims Validation | |
Processing methods |