General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 2.16 g/cm³ Show Material materials with Densidad of 2.16 g/cm³ | DIN EN ISO 12086 |
Densidad aparente | 23.0 °C | 0.76 g/cm³ Show Material materials with Densidad aparente of 0.76 g/cm³ | DIN EN ISO 60 |
Tamaño de partícula | 430000 nm Show Material materials with Tamaño de partícula of 430000 nm | ISO 13320, average value |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 59 [-] Show Material materials with Dureza Shore D of 59 [-] | DIN EN ISO 868 |
Elongación | 23.0 °C | 600 % Show Material materials with Elongación of 600 % | DIN EN ISO 527-3, 0.2 mm film |
Módulo elástico | 23.0 °C | 0.65 GPa Show Material materials with Módulo elástico of 0.65 GPa | DIN EN ISO 527 |
Resistencia a la tracción | 23.0 °C | 35 MPa Show Material materials with Resistencia a la tracción of 35 MPa | DIN EN ISO 527-3, 0.2 mm film |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 1.2E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | ||
200.0 °C | 1.4E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | |||
260.0 °C | 1.7E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | |||
Conductividad térmica | 23.0 °C | 0.22 W/(m·K) Show Material materials with Conductividad térmica of 0.22 W/(m·K) | DIN 52612 | ||
Inflamabilidad | V-0 UL94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 1.00E+16 Ω·m Show Material materials with Resistividad eléctrica of 1.00E+16 Ω·m | IEC 60093 |
Rigidez dieléctrica | 23.0 °C | 82 kV/mm Show Material materials with Rigidez dieléctrica of 82 kV/mm | DIN EN ISO 12086, 0.2 mm film |
Surface resistivity | 23.0 °C | 1.00E+17 Ω/sq Show Material materials with Surface resistivity of 1.00E+17 Ω/sq | IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 3.5 % Show Material materials with Contracción of 3.5 % | Internal Dyneon method, Cylinder 45 mm diameter |
Technological properties
Property | ||
---|---|---|
Application areas | 3M™ Dyneon™ TFM™ Modified PTFE Granules TFM 1610 is suitable for shaped parts, isostatically moulded pump linings or automatic moulded goods enabling applications like static seals for highly demanding pumps or sealing elements for fittings. Furthermore due to its good elasticity the product enables special processing technologies like deep-drawing orblow-moulding. |