General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 2.16 g/cm³ Show Material materials with Densidad of 2.16 g/cm³ | DIN EN ISO 12086 |
Densidad aparente | 23.0 °C | 0.83 g/cm³ Show Material materials with Densidad aparente of 0.83 g/cm³ | DIN EN ISO 60 |
Tamaño de partícula | 230000 nm Show Material materials with Tamaño de partícula of 230000 nm | ISO 13320, average value |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 59 [-] Show Material materials with Dureza Shore D of 59 [-] | DIN EN ISO 868 |
Elongación | 23.0 °C | 600 % Show Material materials with Elongación of 600 % | DIN EN ISO 527-3, 0.2 mm film |
Módulo elástico | 23.0 °C | 0.65 GPa Show Material materials with Módulo elástico of 0.65 GPa | DIN EN ISO 527 |
Resistencia a la tracción | 23.0 °C | 35 MPa Show Material materials with Resistencia a la tracción of 35 MPa | DIN EN ISO 527-3, 0.2 mm film |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 1.2E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature |
200.0 °C | 1.4E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | |
260.0 °C | 1.7E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | |
Conductividad térmica | 23.0 °C | 0.22 W/(m·K) Show Material materials with Conductividad térmica of 0.22 W/(m·K) | DIN 52612 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 1.00E+16 Ω·m Show Material materials with Resistividad eléctrica of 1.00E+16 Ω·m | IEC 60093 |
Rigidez dieléctrica | 23.0 °C | 78 kV/mm Show Material materials with Rigidez dieléctrica of 78 kV/mm | DIN EN ISO 12086, 0.2 mm film |
Surface resistivity | 23.0 °C | 1.00E+17 Ω/sq Show Material materials with Surface resistivity of 1.00E+17 Ω/sq | IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 4.1 % Show Material materials with Contracción of 4.1 % | Internal Dyneon method, Cylinder 45 mm diameter |
Technological properties
Property | ||
---|---|---|
Application areas | 3M™ Dyneon™ TFM™ Modified PTFE Granules TFM 1635 is especially suitable for the manufacturing of shaped parts and large cylinders,forskivedfilms of >250 μm(e.g. aslinings in the chemical processing industry (CPI)), articles requiring improved flexlife properties (diaphragms, bellows etc.), large compression moulded sheets and isostatically moulded articles. |