General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 2.5 g/cm³ Show Material materials with Densidad of 2.5 g/cm³ | ASTM D 4745-06 |
Densidad aparente | 23.0 °C | 0.92 g/cm³ Show Material materials with Densidad aparente of 0.92 g/cm³ | ASTM D 4894-07 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 65 [-] Show Material materials with Dureza Shore D of 65 [-] | DIN 53505 |
Elongación | 23.0 °C | 290 % Show Material materials with Elongación of 290 % | ASTM D 4745-06 |
Resistencia a la tracción | 23.0 °C | 13 MPa Show Material materials with Resistencia a la tracción of 13 MPa | ASTM D 4745-06 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.4 % Show Material materials with Contracción of 1.4 % | ASTM D 4894-07 |
Technological properties
Property | ||
---|---|---|
Application areas | 3MTM DyneonTM PTFE Compound PDR 09001 can be used in sealing applications in the chemical processing (CPI) and automotive industries. | |
Fillers | 10% Carbon Fiber |