General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 2.18 g/cm³ Show Material materials with Densidad of 2.18 g/cm³ | ASTM D 4745-06 |
Densidad aparente | 23.0 °C | 0.81 g/cm³ Show Material materials with Densidad aparente of 0.81 g/cm³ | ASTM D 4894-07 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 67 [-] Show Material materials with Dureza Shore D of 67 [-] | DIN 53505 |
Elongación | 23.0 °C | 300 % Show Material materials with Elongación of 300 % | ASTM D 4745-06 |
Resistencia a la tracción | 23.0 °C | 15.5 MPa Show Material materials with Resistencia a la tracción of 15.5 MPa | ASTM D 4745-06 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.4 % Show Material materials with Contracción of 1.4 % | ASTM D 4894-07 |
Technological properties
Property | ||
---|---|---|
Application areas | 3MTM DyneonTM PTFE Compound TF 6105N can be used in sealing applications in the chemical processing - (CPI) and automotive industry. | |
Fillers | 25% Glass Fiber |