General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 2.06 g/cm³ Show Material materials with Densidad of 2.06 g/cm³ | ASTM D 4745-06 |
Densidad aparente | 23.0 °C | 0.46 g/cm³ Show Material materials with Densidad aparente of 0.46 g/cm³ | ASTM D 4894-07 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 70 [-] Show Material materials with Dureza Shore D of 70 [-] | DIN 53505 |
Elongación | 23.0 °C | 120 % Show Material materials with Elongación of 120 % | ASTM D 4745-06 |
Resistencia a la tracción | 23.0 °C | 19 MPa Show Material materials with Resistencia a la tracción of 19 MPa | ASTM D 4745-06 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.4 % Show Material materials with Contracción of 1.4 % | ASTM D 4894-07 |
Technological properties
Property | ||
---|---|---|
Application areas | 3MTM DyneonTM PTFE Compound TF 7196 can be used in sealing applications in the chemical processing(CPI) and automotive industries. | |
Fillers | 25% Carbon Fiber |