General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad aparente | 23.0 °C | 0.6 g/cm³ Show Material materials with Densidad aparente of 0.6 g/cm³ | ASTM D 1895 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 % Show Material materials with Elongación of 2 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 16 J/m Show Material materials with Impact strength, Izod notched, ASTM of 16 J/m | ASTM D256A |
Módulo de flexión | 23.0 °C | 3.63 GPa Show Material materials with Módulo de flexión of 3.63 GPa | ASTM D 790 |
Módulo elástico | 23.0 °C | 2.99 GPa Show Material materials with Módulo elástico of 2.99 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 66 MPa Show Material materials with Resistencia a la flexión of 66 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 45 MPa Show Material materials with Resistencia a la tracción of 45 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 7 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 7 g/10min | ASTM D 1238 | 200°C/5 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Food Container |