General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad aparente | 23.0 °C | 0.6 g/cm³ Show Material materials with Densidad aparente of 0.6 g/cm³ | ASTM D 1895 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 % Show Material materials with Elongación of 2 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 20 J/m Show Material materials with Impact strength, Izod notched, ASTM of 20 J/m | ASTM D256A |
Módulo de flexión | 23.0 °C | 3.63 GPa Show Material materials with Módulo de flexión of 3.63 GPa | ASTM D 790 |
Módulo elástico | 23.0 °C | 2.99 GPa Show Material materials with Módulo elástico of 2.99 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 95 MPa Show Material materials with Resistencia a la flexión of 95 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 51 MPa Show Material materials with Resistencia a la tracción of 51 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 3.3 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 3.3 g/10min | ASTM D 1238 | 200°C/5 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Food Container |