General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.07 % Show Material materials with Absorción de agua of 0.07 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.32 g/cm³ Show Material materials with Densidad of 1.32 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 % Show Material materials with Elongación of 2 % | ASTM D 638 | Type I, 50 mm/min |
Elongation at yield | 23.0 °C | 2 % Show Material materials with Elongation at yield of 2 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 81 MPa Show Material materials with Flexural yield strength of 81 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 28 J/m Show Material materials with Impact strength, Izod notched, ASTM of 28 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 890 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 890 J/m | ASTM D 4812 |
Límite elástico | 23.0 °C | 50 MPa Show Material materials with Límite elástico of 50 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.29 GPa Show Material materials with Módulo de flexión of 2.29 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.5 GPa Show Material materials with Módulo elástico of 2.5 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la tracción | 23.0 °C | 50 MPa Show Material materials with Resistencia a la tracción of 50 MPa | ASTM D 638 | Type I, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 7 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | ISO 179/1eA |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 2 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 2 kJ/m² | ISO 180/1A |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 35 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 35 kJ/m² | ISO 180/1U |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 8.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 8.5E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 8.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 8.5E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Heat deflection temperature, 0.45 MPa | 113 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 113 °C | ISO 75/Bf | 0.45 MPa | |
Temperatura de reblandecimiento Vicat | 177 °C Show Material materials with Temperatura de reblandecimiento Vicat of 177 °C | ISO 306 | Rate B/120 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.5 - 1.8 % Show Material materials with Contracción of 1.5 - 1.8 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 1.6 - 2 % Show Material materials with Contracción transversal of 1.6 - 2 % | SABIC method |
Velocidad de flujo de la masa derretida | 127 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 127 g/10min | ASTM D 1238 | 250°C/1.2 kgf | |
Velocidad de flujo del volumen derretido | 231 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 231 cm³/10min | ISO 1133 | 250°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Protection,Heavy Vehicles,Pharmaceutical Manufacturing,Water Treatment/Filtration | |
Processing methods | Drying Temperature: 110-120°C, Drying Time: 4-6hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 245-260°C, Barrel - Zone 1 Temperature: 200-230°C, Barrel - Zone 2 Temperature: 240-255°C, Barrel - Zone 3 Temperature: 240-275°C, Barrel - Zone 4 Temperature: 240-275°C, Adapter Temperature: 240-275°C, Die Temperature: 240-275°C |