General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.08 % Show Material materials with Absorción de agua of 0.08 % | ASTM D 570 | 24 Hours |
Densidad | 23.0 °C | 1.31 g/cm³ Show Material materials with Densidad of 1.31 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 300 % Show Material materials with Elongación of 300 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 82 MPa Show Material materials with Flexural yield strength of 82 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Hardness, Rockwell R | 23.0 °C | 117 [-] Show Material materials with Hardness, Rockwell R of 117 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 53 J/m Show Material materials with Impact strength, Izod notched, ASTM of 53 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1602 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 1602 J/m | ASTM D 4812 |
Límite elástico | 23.0 °C | 51 MPa Show Material materials with Límite elástico of 51 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.34 GPa Show Material materials with Módulo de flexión of 2.34 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Resistencia a la flexión | 23.0 °C | 82 MPa Show Material materials with Resistencia a la flexión of 82 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 51 MPa Show Material materials with Resistencia a la tracción of 51 MPa | ASTM D 638 | Type I, 50 mm/min |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.39E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.39E-4 1/K | ASTM E 831 | 60°C to 138°C | ||
Heat deflection temperature, 1.80 MPa | 54 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 54 °C | ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed | |||
Relative temperature index, electrical | 120 °C Show Material materials with Relative temperature index, electrical of 120 °C | UL 746B | |||
Relative temperature index, mechanical impact | 120 °C Show Material materials with Relative temperature index, mechanical impact of 120 °C | UL 746B | |||
Relative temperature index, mechanical strength | 140 °C Show Material materials with Relative temperature index, mechanical strength of 140 °C | UL 746B | |||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating | 1.47mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3.1 [-] Show Material materials with Constante dieléctrica of 3.1 [-] | ASTM D 150 | at 1 MHz |
Factor de disipación | 23.0 °C | 0.02 [-] Show Material materials with Factor de disipación of 0.02 [-] | ASTM D 150 | at 1 MHz |
Rigidez dieléctrica | 23.0 °C | 15.7 kV/mm Show Material materials with Rigidez dieléctrica of 15.7 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 0 V Show Material materials with Índice de seguimiento comparativo of 0 V | UL 746A |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.5 - 2.3 % Show Material materials with Contracción of 1.5 - 2.3 % | SABIC method | 2.3-4.6 mm |
Contracción transversal | 23.0 °C | 1.6 - 2.4 % Show Material materials with Contracción transversal of 1.6 - 2.4 % | SABIC method | 2.3-4.6 mm |
Melt viscosity | 23.0 °C | 600 Pa·s Show Material materials with Melt viscosity of 600 Pa·s | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Audio,Auto Aftermarket,Circuit Protection,Document Handling,Electronic Components,Enclosures,Food Container,Freezer,Gas/Electric Oven,Hygiene/Personal Care,Lawn/Garden,Medical Device,Medical Facility Infrastructure,Non-LED Lighting,Personal Computing,Plumbing,Recreational Vehicle,Refrigerator,Semiconductor,Swimming Pool/Spa,Wireless Communications,Wiring Devices | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 12hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 245-260°C, Nozzle Temperature: 240-255°C, Front - Zone 3 Temperature: 245-260°C, Middle - Zone 2 Temperature: 240-255°C, Rear - Zone 1 Temperature: 230-250°C, Mold Temperature: 50-75°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 50-100rpm, Shot to Cylinder Size: 40-80%, Vent Depth: 0.013-0.025mm |