General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad aparente | 23.0 °C | 0.6 g/cm³ Show Material materials with Densidad aparente of 0.6 g/cm³ | ASTM D 1895 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 50 % Show Material materials with Elongación of 50 % | ASTM D638 |
Hardness, Rockwell L | 23.0 °C | 60 [-] Show Material materials with Hardness, Rockwell L of 60 [-] | ASTM D785 |
Módulo de flexión | 23.0 °C | 2.35 GPa Show Material materials with Módulo de flexión of 2.35 GPa | ASTM D 790 |
Módulo elástico | 23.0 °C | 2.16 GPa Show Material materials with Módulo elástico of 2.16 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 35 MPa Show Material materials with Resistencia a la flexión of 35 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 22 MPa Show Material materials with Resistencia a la tracción of 22 MPa | ASTM D638 |
Aplicaciones térmicas
Technological properties
Property | ||
---|---|---|
Application areas | Air Conditioning,Amusement Machine,ATM/Ticket Machine,Auto Aftermarket,Circuit Protection,Cluster,Console,Cooking Range,Data Transfer,Dishwasher,Document Handling,Door Handle,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Exterior Mirror,Fluid Delivery,Food Transportation,Forward Lighting,Gas/Electric Oven,Heavy Vehicles,Hygiene/Personal Care,Laundry Dryer,Lawn/Garden,LED Lighting,Medical Device,Meter Gas,Meter Water,Monitoring and Imaging,Motorcycle,Non-LED Lighting,Personal Computing,Power Manangement,Rear/Signal Lighting,Refrigerator,Respiratory,Small Appliance,Surgical Devices,Swimming Pool/Spa,Trim,Watch/Jewelry,Wireless Communications,Wiring Devices,Irrigation,Wire & cable |