General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.14 % Show Material materials with Absorción de agua of 0.14 % | ASTM D 570 | 24 Hours |
Absorción de agua, equilibrio | 23.0 °C | 0.6 % Show Material materials with Absorción de agua, equilibrio of 0.6 % | ASTM D 570 |
Densidad | 23.0 °C | 1.33 g/cm³ Show Material materials with Densidad of 1.33 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 120 % Show Material materials with Elongación of 120 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 68 MPa Show Material materials with Flexural yield strength of 68 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Hardness, Rockwell R | 23.0 °C | 115 [-] Show Material materials with Hardness, Rockwell R of 115 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | -40.0 °C | 170 J/m Show Material materials with Impact strength, Izod notched, ASTM of 170 J/m | ASTM D 256 |
-30.0 °C | 192 J/m Show Material materials with Impact strength, Izod notched, ASTM of 192 J/m | ASTM D 256 | |
23.0 °C | 640 J/m Show Material materials with Impact strength, Izod notched, ASTM of 640 J/m | ASTM D 256 | |
Límite elástico | 23.0 °C | 41 MPa Show Material materials with Límite elástico of 41 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.24 GPa Show Material materials with Módulo de flexión of 2.24 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Resistencia a la flexión | 23.0 °C | 68 MPa Show Material materials with Resistencia a la flexión of 68 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 41 MPa Show Material materials with Resistencia a la tracción of 41 MPa | ASTM D 638 | Type I, 50 mm/min |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 8.28E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 8.28E-5 1/K | ASTM E 831 | 60°C to 138°C | ||
Heat deflection temperature, 1.80 MPa | 121 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 121 °C | ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed | |||
Relative temperature index, electrical | 105 °C Show Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Inflamabilidad | UL Recognized, 94-5VA Flame Class Rating | 2.2mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 5.7 [-] Show Material materials with Constante dieléctrica of 5.7 [-] | ASTM D 150 | at 1 MHz |
Factor de disipación | 23.0 °C | 0.03 [-] Show Material materials with Factor de disipación of 0.03 [-] | ASTM D 150 | at 1 MHz |
Rigidez dieléctrica | 23.0 °C | 12 kV/mm Show Material materials with Rigidez dieléctrica of 12 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 3 V Show Material materials with Índice de seguimiento comparativo of 3 V | UL 746A |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1 - 1.4 % Show Material materials with Contracción of 1 - 1.4 % | SABIC method | 2.3-4.6 mm |
Contracción transversal | 23.0 °C | 1.2 - 1.6 % Show Material materials with Contracción transversal of 1.2 - 1.6 % | SABIC method | 2.3-4.6 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Protection,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Heavy Vehicles,Medical Device,Personal Computing,Surgical Devices,Wireless Communications | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 12hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 250-265°C, Nozzle Temperature: 245-260°C, Front - Zone 3 Temperature: 250-265°C, Middle - Zone 2 Temperature: 245-260°C, Rear - Zone 1 Temperature: 240-255°C, Mold Temperature: 50-75°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 50-100rpm, Shot to Cylinder Size: 40-80%, Vent Depth: 0.025-0.038mm |