General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.07 % Show Material materials with Absorción de agua of 0.07 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.59 g/cm³ Show Material materials with Densidad of 1.59 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Material materials with Elongación of 3 % | ASTM D 638 | Type I, 5 mm/min |
Elongation at yield | 23.0 °C | 2 % Show Material materials with Elongation at yield of 2 % | ASTM D 638 | Type I, 5 mm/min |
Flexural strain | 23.0 °C | 3 % Show Material materials with Flexural strain of 3 % | ISO 178 | 2 mm/min |
Flexural yield strength | 23.0 °C | 205 MPa Show Material materials with Flexural yield strength of 205 MPa | ISO 178 | 2 mm/min |
Hardness, Ball Indentation | 23.0 °C | 132 MPa Show Material materials with Hardness, Ball Indentation of 132 MPa | ISO 2039-1 |
Hardness, Rockwell R | 23.0 °C | 118 [-] Show Material materials with Hardness, Rockwell R of 118 [-] | ISO 2039-2 |
Impact strength, Izod notched, ASTM | -30.0 °C | 90 J/m Show Material materials with Impact strength, Izod notched, ASTM of 90 J/m | ASTM D 256 |
23.0 °C | 85 J/m Show Material materials with Impact strength, Izod notched, ASTM of 85 J/m | ASTM D 256 | |
Impact strength, Izod unnotched, ASTM | -30.0 °C | 770 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 770 J/m | ASTM D 4812 |
23.0 °C | 640 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 640 J/m | ASTM D 4812 | |
Límite elástico | 23.0 °C | 140 MPa Show Material materials with Límite elástico of 140 MPa | ASTM D 638 | Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 9.5 GPa Show Material materials with Módulo de flexión of 9.5 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 10.7 GPa Show Material materials with Módulo elástico of 10.7 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 200 MPa Show Material materials with Resistencia a la flexión of 200 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 110 MPa Show Material materials with Resistencia a la tracción of 110 MPa | ASTM D 638 | Type I, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 11 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | ISO 179/2C |
23.0 °C | 11 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | ISO 179/2C | |
Resistencia al choque, ensayo Charpy no entallado | -30.0 °C | 55 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 55 kJ/m² | ISO 179/2C |
23.0 °C | 60 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | ISO 179/2C | |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 9 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 9 kJ/m² | ISO 180/1A |
23.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 10 kJ/m² | ISO 180/1A | |
Resistencia al choque, ensayo Izod no entallado | -30.0 °C | 52 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 52 kJ/m² | ISO 180/1U |
23.0 °C | 53 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 53 kJ/m² | ISO 180/1U | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 5.77E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 5.77E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 1.80 MPa | 138 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 138 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Relative temperature index, electrical | 125 °C Show Material materials with Relative temperature index, electrical of 125 °C | UL 746B | |||
Relative temperature index, mechanical impact | 110 °C Show Material materials with Relative temperature index, mechanical impact of 110 °C | UL 746B | |||
Relative temperature index, mechanical strength | 125 °C Show Material materials with Relative temperature index, mechanical strength of 125 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 165 °C Show Material materials with Temperatura de reblandecimiento Vicat of 165 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | Needle Flame Test, 10 s , passes at | 1.5mm | IEC 60695-2-2 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3.4 [-] Show Material materials with Constante dieléctrica of 3.4 [-] | IEC 60250 | at 50/60 Hz |
Factor de disipación | 23.0 °C | 0.02 [-] Show Material materials with Factor de disipación of 0.02 [-] | IEC 60250 | at 2450 MHz |
Rigidez dieléctrica | 23.0 °C | 15 kV/mm Show Material materials with Rigidez dieléctrica of 15 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 225 V Show Material materials with Índice de seguimiento comparativo of 225 V | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.5 - 0.9 % Show Material materials with Contracción transversal of 0.5 - 0.9 % | SABIC method |
Melt viscosity | 260.0 °C | 200 Pa·s Show Material materials with Melt viscosity of 200 Pa·s | ISO 11443 | 1500 sec⁻¹ |
Velocidad de flujo de la masa derretida | 40 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 40 g/10min | ASTM D 1238 | 266°C/5.0 kg | |
Velocidad de flujo del volumen derretido | 30 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 30 cm³/10min | ISO 1133 | 265°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Air Conditioning,Building Accessory,Circuit Protection,Cladding/Roof,Coffee Maker/Espresso Machine,Data Management,Data Transfer,Displays,Document Handling,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Exterior Trim,Gas/Electric Oven,Heavy Vehicles,Lab Ware and Clinical Diagnostics,LED Lighting,Medical Device,Medical Facility Infrastructure,Meter Gas,Non-LED Lighting,Personal Care,Personal Computing,Photovoltaic Components,Power Manangement,Pump,Rail,Security/Detection,Semiconductor,Trim,Wireless Communications,Wiring Devices,Wire & cable | |
Fillers | 30% Glass Fiber | |
Processing methods | Drying Temperature: 110-120°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 250-270°C, Nozzle Temperature: 240-260°C, Front - Zone 3 Temperature: 245-265°C, Middle - Zone 2 Temperature: 240-255°C, Rear - Zone 1 Temperature: 230-245°C, Hopper Temperature: 40-60°C, Mold Temperature: 40-100°C |