General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 150 % Show Material materials with Elongación of 150 % | ASTM D 638 | Type I, 50 mm/min |
Elongation at yield | 23.0 °C | 5 % Show Material materials with Elongation at yield of 5 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 75 MPa Show Material materials with Flexural yield strength of 75 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | -30.0 °C | 530 J/m Show Material materials with Impact strength, Izod notched, ASTM of 530 J/m | ASTM D 256 |
23.0 °C | 747 J/m Show Material materials with Impact strength, Izod notched, ASTM of 747 J/m | ASTM D 256 | |
Límite elástico | 23.0 °C | 51 MPa Show Material materials with Límite elástico of 51 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 1.9 GPa Show Material materials with Módulo de flexión of 1.9 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 1.89 GPa Show Material materials with Módulo elástico of 1.89 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la tracción | 23.0 °C | 50 MPa Show Material materials with Resistencia a la tracción of 50 MPa | ASTM D 638 | Type I, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 57 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 57 kJ/m² | ISO 179/1eA |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 42 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 42 kJ/m² | ISO 180/1A |
23.0 °C | 50 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 50 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.71E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.71E-4 1/K | ASTM E 831 | -40°C to 40°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 2E-4 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 2E-4 1/K | ASTM E 831 | -40°C to 40°C |
Heat deflection temperature, 1.80 MPa | 87 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 87 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |
Temperatura de reblandecimiento Vicat | 125 °C Show Material materials with Temperatura de reblandecimiento Vicat of 125 °C | ASTM D 1525 | Rate B/50 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.8 - 1 % Show Material materials with Contracción of 0.8 - 1 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 13 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 13 g/10min | ASTM D 1238 | 250°C/5.0 kgf | |
Velocidad de flujo del volumen derretido | 26 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 26 cm³/10min | ISO 1133 | 220°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components,Enclosure/Housing/Cover,Vacuum Cleaner | |
Processing methods | Drying Temperature: 110°C, Drying Time: 4-6hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 255-275°C, Nozzle Temperature: 250-265°C, Front - Zone 3 Temperature: 250-270°C, Middle - Zone 2 Temperature: 245-265°C, Rear - Zone 1 Temperature: 240-260°C, Mold Temperature: 40-90°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-80rpm, Shot to Cylinder Size: 50-80%, Vent Depth: 0.013-0.02mm |