General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.2 g/cm³ Show Material materials with Densidad of 1.2 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 175 % Show Material materials with Elongación of 175 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 64 MPa Show Material materials with Flexural yield strength of 64 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched, ASTM | 23.0 °C | 850 J/m Show Material materials with Impact strength, Izod notched, ASTM of 850 J/m | ASTM D 256 |
Límite elástico | 23.0 °C | 43 MPa Show Material materials with Límite elástico of 43 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 1.72 GPa Show Material materials with Módulo de flexión of 1.72 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 60 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 60 °C | ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.5 - 2 % Show Material materials with Contracción of 1.5 - 2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components,Enclosures,Heavy Vehicles,Lawn/Garden,Monitoring and Imaging,Security/Detection | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 12hrs, Melt Temperature: 250-290°C, Mold Temperature: 55-80°C |