General
Property | Value | Comment |
---|---|---|
Densidad | 0.902 g/cm³ Show Material materials with Densidad of 0.902 g/cm³ | ASTM D1505 |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 850.0 % Show Material materials with Elongación of 850.0 % | ASTM D638 |
Módulo de flexión | 0.0744799999999999 GPa Show Material materials with Módulo de flexión of 0.0744799999999999 GPa | ASTM D790 |
Resistencia a la tracción | 19.6 MPa Show Material materials with Resistencia a la tracción of 19.6 MPa | ASTM D638 |
Aplicaciones térmicas
Óptico
Property | Value | Comment |
---|---|---|
Turbidez | 0.5 % Show Material materials with Turbidez of 0.5 % | ASTM D1003 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Viscosidad mooney | 10.0 MU Show Material materials with Viscosidad mooney of 10.0 MU | ASTM D1646 | ML 1+4, 121 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Stretch film,General purpose film,Lamination film |