General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 143 % Show Material materials with Elongación of 143 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 97 MPa Show Material materials with Flexural yield strength of 97 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched, ASTM | 23.0 °C | 801 J/m Show Material materials with Impact strength, Izod notched, ASTM of 801 J/m | ASTM D 256 |
Límite elástico | 23.0 °C | 65 MPa Show Material materials with Límite elástico of 65 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Material materials with Módulo de flexión of 2.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 133 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 133 °C | ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 - 0.7 % Show Material materials with Contracción of 0.5 - 0.7 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 18 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 18 g/10min | ASTM D 1238 | 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Protection,Data Transfer,Displays,Electronic Components,Enclosures,Energy Management,LED Lighting,Medical Device,Medical Facility Infrastructure,Non-LED Lighting,Surgical Devices,Wiring Devices | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 48hrs, Melt Temperature: 280-305°C, Mold Temperature: 70-95°C |