General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.93 g/cm³ Show Material materials with Densidad of 0.93 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 48 [-] Show Material materials with Dureza Shore D of 48 [-] | ASTM D2240 |
Elongación | 23.0 °C | 850 % Show Material materials with Elongación of 850 % | ASTM D638 |
Elongation at yield | 23.0 °C | 12 % Show Material materials with Elongation at yield of 12 % | ISO 527-1/-2 |
Límite elástico | 23.0 °C | 14 MPa Show Material materials with Límite elástico of 14 MPa | ASTM D638 |
Resistencia a la tracción | 23.0 °C | 25 MPa Show Material materials with Resistencia a la tracción of 25 MPa | ASTM D638 |
Eléctrico
Technological properties
Property | ||
---|---|---|
Application areas | Electrical,Wire & cable |