General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.92 g/cm³ Show Material materials with Densidad of 0.92 g/cm³ | ASTM D1505 |
Mecánica
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 2.17 [-] Show Material materials with Constante dieléctrica of 2.17 [-] | ASTM D150 | at 60 Hz |
Factor de disipación | 23.0 °C | 1000 [-] Show Material materials with Factor de disipación of 1000 [-] | ASTM D150 | at 60 Hz |
Resistividad eléctrica | 23.0 °C | 5.00E+13 Ω·m Show Material materials with Resistividad eléctrica of 5.00E+13 Ω·m | ASTM D257 |
Rigidez dieléctrica | 23.0 °C | 55 kV/mm Show Material materials with Rigidez dieléctrica of 55 kV/mm | ASTM D149 | at 500 V/sec |
Óptico
Property | Value | Comment |
---|---|---|
Turbidez | 1.2 % Show Material materials with Turbidez of 1.2 % | ASTM D1003 |
Technological properties
Property | ||
---|---|---|
Application areas | It is typically used for food applications (lamination film, barrier film) but can also be used in industrial packaging and as blending partner with other SABIC® PE resins in both blown and cast film applications. |