Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.41 g/cm³ Show Material materials with Densidad of 1.41 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation at yield | 23.0 °C | 11 % Show Material materials with Elongation at yield of 11 % | ISO 527-2 1A | 50mm/min |
Límite elástico | 23.0 °C | 61 MPa Show Material materials with Límite elástico of 61 MPa | ISO 527-2 1A | 50 mm/min |
Módulo de flexión | 23.0 °C | 2.5 GPa Show Material materials with Módulo de flexión of 2.5 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 2.4 GPa Show Material materials with Módulo elástico of 2.4 GPa | ISO 527-2 1A | 1mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 8.5 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 8.5 kJ/m² | ISO 179/1eA |
Aplicaciones térmicas
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo del volumen derretido | 2.5 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 2.5 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive |