General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.92 g/cm³ Show Material materials with Densidad of 0.92 g/cm³ | ASTM D1505 |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 120 °C Show Material materials with Temperatura de fusión of 120 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 2.25 [-] Show Material materials with Constante dieléctrica of 2.25 [-] | ASTM D150 |
Factor de disipación | 23.0 °C | 7E-4 [-] Show Material materials with Factor de disipación of 7E-4 [-] | ASTM D150 |
Rigidez dieléctrica | 23.0 °C | 37 kV/mm Show Material materials with Rigidez dieléctrica of 37 kV/mm | ASTM D150 |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable |